Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Polycasa Acryl® KR 2015/1 Acrylic, Impact Grade Medium-impact grade with very good flow behavior, especially mechanically stressed parts with long flow paths; e.g. strip light diffusers. Can be extruded into thin tubes, sheet and film.Data was c.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® 2783, Extrusion Grade
(discontinued **) Extrusion grade with super high impact.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majority shareholding under a J.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Ineos ABS Lustran® QE 1006, Extrusion Grade
(discontinued **) Extrusion grade with high impact.Applications: High impact plates.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEOS acquires a majo.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Oroglas® DRT Acrylic, Impact Grade
(discontinued **) For extrusion and injection molding applications. OROGLAS DRT combines good thermal resistance with an excellent impact resistance.Key features : impact resistance: up to 10 times more impact-resis.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ASTM D696 |
Solvay Specialty Polymers Halar® 901 Polyethylene, Chlorotrifluoroethylene (ECTFE)
(Unverified Data**)< Information provided by Solvay Specialty Polymers. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1,-2 |
Lanxess Durethan® BC 30 S 000000 Nylon 6 PA 6, non-reinforced, injection moldingInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 23.0 - 55.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-1, -2 |
Lanxess Pocan® B 5220 XF 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, improved flowability, improved impact strength, low tendency to warpInformation provided by LANXESS. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Solvay Specialty Polymers Halar® 5001C Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Powder grades for masterbatches.Features: Low ViscosityUses: Masterbatch; Wire & Cable ApplicationsAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | |
Solvay Specialty Polymers Halar® 930LCW Ethylene Chlorotrifluoroethylene Copolymer (ECTFE) Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3418 40.0 J/g; Heat of Fusion - ASTM D3418 42.0 J/g; Thermal Stability - TGA 405 °CInformation provided by Solvay Specialty Pol.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359 |
Styrolution Terblend® N NM-11 ABS/PA6 (Dry) Terblend N NM-11 is an ABS/PA6 blend combining very high impact strength, even at low temperatures, with an excellent processability and surface appearance.Information provided by STYROLUTION, which.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
DSM Akulon® F160-Z PA6 Very High Viscosity, Lubricated |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
ISO 11359-1/-2 |
DSM Akulon® K240-HP Impact Modified Nylon 6 (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C | 55.6 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® E53 NC010 Nylon 66 Unreinforced High Viscosity Polyamide 66 Information provided by DuPont Performance Polymers |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature -40.0 - 23.0 °C |
55.6 µin/in-°F @Temperature -40.0 - 73.4 °F |
ISO 11359-1/-2 |
DuPont Performance Polymers Delrin® 500PE NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE NC010 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 23.0 - 60.0 °C |
55.6 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
Eurostar Staramide R1000HI620 PA66, Impact Modified, Injection Molded Staramide R1000HI620 is an Impact Modified Polyamide 66 Injection Molding Resin (also known as R1000HI010)Information provided by Eurostar. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 445 E WU Impact Grade Polystyrene (Europe) Easy flowing, heat-resistant, medium-impact, flame-retardant grade. Application example: electrical distribution boxes.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 456 F Impact Grade Polystyrene (Europe) Heat distortion resistant, good flowing grade for parts subjected to heat.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 475 K Impact Grade Polystyrene (Europe) Normal flowing, high-impact grade with particularly good creep strength.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
BASF Polystyrol® 585 K Impact Grade Polystyrene (Europe) Special high gloss, high-impact grade for all types of housings. Basis product for gloss capping.Data was collected by ISO methods and provided by BASF. |
|||
CTE, linear, Parallel to Flow | 100 µm/m-°C @Temperature 20.0 °C |
55.6 µin/in-°F @Temperature 68.0 °F |
|
Arkema Group Oroglas® SG 10 Acrylic, Gamma Radiation Resistant
(discontinued **) OROGLAS SG 10 is special Gamma - radiation - resistant formulation designed for use in medical devises.OROGLAS SG 10 maintains exceptional clarity after 5 megarads of Gamma radiation with no advers.. |