Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 4.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
2.22 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D696 |
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66 LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant. |
|||
CTE, linear, Parallel to Flow | 4.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
2.22 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
CTE, linear, Parallel to Flow | 4.00 µm/m-°C @Temperature -30.0 - 30.0 °C |
2.22 µin/in-°F @Temperature -22.0 - 86.0 °F |
ASTM D 696 |
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region.. |
|||
CTE, linear, Parallel to Flow | 4.00 µm/m-°C @Temperature 23.0 - 60.0 °C |
2.22 µin/in-°F @Temperature 73.4 - 140 °F |
ISO 11359-2 |
SABIC Innovative Plastics LNP THERMOCOMP LC008EXP PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LC008EXP is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include Electrically Conductive, Easy Molding. |
|||
CTE, linear, Parallel to Flow | 4.00 µm/m-°C | 2.22 µin/in-°F | TMA |
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic VYNTEC CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several o.. |
|||
CTE, linear, Parallel to Flow | 4.00 µm/m-°C | 2.22 µin/in-°F | DAM; ISO 11359-1/-2 |
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
CTE, linear, Parallel to Flow | 4.00 - 5.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
2.22 - 2.78 µin/in-°F @Temperature 73.4 - 176 °F |
|
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |
|||
CTE, linear, Parallel to Flow | 4.00 µm/m-°C @Temperature 23.0 - 55.0 °C |
2.22 µin/in-°F @Temperature 73.4 - 131 °F |
DIN 53752 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
CTE, linear, Parallel to Flow | 4.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
2.22 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur S 4090 G4 20% Glass Filled PBT Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio.. |
|||
CTE, linear, Parallel to Flow | 4.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
2.22 µin/in-°F @Temperature 73.4 - 176 °F |
DIN 53752 |
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs.. |