Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic , Phenolic, Carbon Fiber Composite
Manufacturer Vyncolit N.V., Sumitomo Bakelite
Trade Name Vyntec®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
VYNTEC CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several oils. Datasheet is based on postcured test specimens.Information provided by Sumitomo Bak North America, Inc.
Physical Properties Metric English Comments
Bulk Density 0.570 g/cc
0.0206 lb/in³
ISO 60
Density 1.46 g/cc
0.0527 lb/in³
ISO 1183
Water Absorption 0.10 %
0.10 %
ISO 62
Linear Mold Shrinkage 0.00020 cm/cm
0.00020 in/in
ISO 2577
Mechanical Properties Metric English Comments
Tensile Strength at Break 108 MPa
15700 psi
ISO 527-1
Elongation at Break 0.40 %
0.40 %
ISO 527-1
Tensile Modulus 31.0 GPa
4500 ksi
ISO 527-1
Flexural Strength 239 MPa
34700 psi
ISO 178
Flexural Modulus 28.0 GPa
4060 ksi
ISO 178
Compressive Strength 200 MPa
29000 psi
ISO 604
Charpy Impact Unnotched 1.09 J/cm²
5.19 ft-lb/in²
ISO 179-1
Charpy Impact, Notched 0.280 J/cm²
1.33 ft-lb/in²
ISO 179-1
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 4.00 µm/m-°C
2.22 µin/in-°F
TMA
CTE, linear, Transverse to Flow 27.0 µm/m-°C
15.0 µin/in-°F
TMA
Deflection Temperature at 1.8 MPa (264 psi) >= 250 °C
>= 482 °F
ISO 75 Af
Shrinkage 0.020 %
0.020 %
Post Shrinkage; ISO 2577
Descriptive Properties Value Comments
Color Black
Molding Method Compression
Injection
Transfer
Users viewing this material also viewed the following: