Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
2.22 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D696
SABIC Innovative Plastics LNP LUBRILOY RA2 PA 66
LNP* LUBRILOY* RA2 is a compound based on Nylon 66 resin containing Aramid Fiber. Added feature of this material is: Wear Resistant.
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
2.22 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS
LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region.
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature -30.0 - 30.0 °C
2.22 µin/in-°F

@Temperature -22.0 - 86.0 °F
ASTM D 696
SABIC Innovative Plastics LNP Thermocomp DFZ22E PC
LNP* Thermocomp* DFZ22E is a compound based on Polycarbonate with Glass and Milled Fiber. Characteristics of this products is Easy Molding.This data was supplied by SABIC-IP for the Americas region..
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature 23.0 - 60.0 °C
2.22 µin/in-°F

@Temperature 73.4 - 140 °F
ISO 11359-2
SABIC Innovative Plastics LNP THERMOCOMP LC008EXP PEEK (Europe-Africa-Middle East)
LNP* THERMOCOMP* LC008EXP is a compound based on Polyetheretherketone containing Carbon Fiber. Added features include Electrically Conductive, Easy Molding.
CTE, linear, Parallel to Flow 4.00 µm/m-°C
2.22 µin/in-°F
TMA
Vyncolit Vyntec® CF8131 Carbon Fiber Reinforced Phenolic
VYNTEC CF8050 is a carbon fiber reinforced phenolic moldable composite with good tribological and superior mechanical properties combined with low density. Very good chemical resistance in several o..
CTE, linear, Parallel to Flow 4.00 µm/m-°C
2.22 µin/in-°F
DAM; ISO 11359-1/-2
DuPont Performance Polymers Zytel® 73G30T BK261 Nylon 6  (Unverified Data**)
30% Glass Reinforced Toughened Polyamide 6 Zytel 73G30T BK261 is a 30% glass fiber reinforced toughened black polyamide 6 resin for injection molding.Information provided by DuPont Performance Polym..
CTE, linear, Parallel to Flow 4.00 - 5.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
2.22 - 2.78 µin/in-°F

@Temperature 73.4 - 176 °F
BASF Ultradur B 4300 G2 10% Glass Filled PBT
Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature 23.0 - 55.0 °C
2.22 µin/in-°F

@Temperature 73.4 - 131 °F
DIN 53752
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM
Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness.
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
2.22 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur S 4090 G4 20% Glass Filled PBT
Ultradur S 4090 G4 is a 20% glass reinforced PBT+ASA blend. It produces moldings with good surface finish,is resistant to chemicals and stress cracking, and has low shrinkage and warpage.Applicatio..
CTE, linear, Parallel to Flow 4.00 µm/m-°C

@Temperature 23.0 - 80.0 °C
2.22 µin/in-°F

@Temperature 73.4 - 176 °F
DIN 53752
BASF Ultradur® B 4300 GM42 20/10% Glass/Mineral Filled PBT
Description: Is a PBT-HI, mixed glass-fiber-reinforced and mineral-reinforced injection-molding grade with good surface quality and rigidity, and with low warpage for parts such as housings and PCBs..