Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear, Parallel to Flow | 1.00 - 5.00 µm/m-°C @Temperature 20.0 °C |
0.556 - 2.78 µin/in-°F @Temperature 68.0 °F |
TMA |
Vyncolit Vyntec® CF8030 Carbon Fiber Reinforced Novolac Phenolic Carbon fiber reinforced phenolic moldable composite with superior tribological properties. High tensile and flexural strength and modulus combined with low density.Information provided by Vyncolit,.. |
|||
CTE, linear, Parallel to Flow | 4.00 - 5.00 µm/m-°C @Temperature 23.0 - 80.0 °C |
2.22 - 2.78 µin/in-°F @Temperature 73.4 - 176 °F |
|
BASF Ultradur B 4300 G2 10% Glass Filled PBT Ultradur B4300 G2 is an easy flowing injection molding PBT with 10% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small.. |