Thermal Properties Metric English Comments
Heat of Fusion 57.0 J/g
24.5 BTU/lb
ASTM E793
Eastman CM01 PET  (discontinued **)
Voridian Polymer CM01 is clear polymer that is available in North America. This product is useful for production of beverage, food, and edible oil containers.Applications/UsesCarbonated soft drink c..
Heat of Fusion 57.0 J/g
24.5 BTU/lb
ASTM E793
Eastman GP800 PET  (discontinued **)
Voridian PET GP800 is a general purpose polymer that is available in the European, Middle East and Africa region. This product is developed for optimal production of PET bottles, containers, and fil..
Heat of Fusion 57.0 - 66.0 J/g
24.5 - 28.4 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Heat of Fusion 57.0 - 66.0 J/g
24.5 - 28.4 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Heat of Fusion 57.0 - 66.0 J/g
24.5 - 28.4 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.