Thermal Properties | Metric | English | Comments |
---|---|---|---|
Heat of Fusion | 57.0 - 66.0 J/g | 24.5 - 28.4 BTU/lb | ASTM D3417 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 57.0 - 66.0 J/g | 24.5 - 28.4 BTU/lb | ASTM D3417 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers. |
|||
Heat of Fusion | 57.0 - 66.0 J/g | 24.5 - 28.4 BTU/lb | ASTM D3417 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |