Polymer Property : Heat of Fusion = 28.4 BTU/lb Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Heat of Fusion 57.0 - 66.0 J/g
24.5 - 28.4 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.
Heat of Fusion 57.0 - 66.0 J/g
24.5 - 28.4 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Information provided by Solvay Specialty Polymers.
Heat of Fusion 57.0 - 66.0 J/g
24.5 - 28.4 BTU/lb
ASTM D3417
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF)  (Unverified Data**)
Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Information provided by Solvay Specialty Polymers.