Material Notes:
PERMABOND 200 is a high viscosity product with good flow control useful in wire tacking applications or bonding components. It is fast setting and suitable for use on plastics, rubber and metals. Cyanoacrylate adhesives are single component adhesives that polymerize rapidly when pressed into a thin film between parts. The moisture adsorbed on the surface initiates the curing of the adhesive. Strong bonds are developed extremely fast and on a great variety of materials. These properties make PERMABOND cyanoacrylates the ideal adhesives for high speed production lines. Features and Benefits: Fast setting and fixturing of parts Rapid development of high strength Ease of use-no mixing, no heat cure Bonds most materials 100% reactive, no solvents Typical Applications: Wire tacking Component Mounting Encapsulating Soluble in Nitroethane, Methyl Ethyl Ketone, and Acetone.Information provided by Permabond.
Physical Properties Metric English Comments
Specific Gravity 1.05 g/cc
1.05 g/cc
Uncured
Viscosity 1500 cP

@Temperature 25.0 °C
1500 cP

@Temperature 77.0 °F
Uncured
Storage Temperature 2.00 - 7.00 °C
35.6 - 44.6 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 85
85
Adhesive Bond Strength 8.30 MPa
1200 psi
Aluminum, Shear
22.0 MPa
3190 psi
Grit-blasted Steel, Shear
Impact 6.3 - 14.7
6.3 - 14.7
kJ/m<sup>2</sup> Adhesive Impact Strength; ASTM D950
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 82.0 °C
180 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Flash Point 83.0 °C
181 °F
Electrical Properties Metric English Comments
Dielectric Strength 9.84 kV/mm
250 kV/in
Processing Properties Metric English Comments
Cure Time 0.250 min
0.00417 hour
Steel, set time
0.250 min
0.00417 hour
Buna N Rubber, set time
0.250 min
0.00417 hour
Phenolic, set time
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
full strength
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance Colorless
Uncured
Maximum Gap Fill (mm) 0.38