Tra-Con Tra-Bond FS443 Color Keyed Thixotropic Epoxy Adhesive

Category Polymer , Adhesive , Thermoset , Epoxy
Manufacturer Tra-Con, Inc.
Trade Name Tra-Bond
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tra-Con Tra-Bond FS443 Color Keyed Thixotropic Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
TRA-BOND FS443 is a fast cure, high viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating single or multi-channel fiber optic connectors. Although this unique three-step color-change formulation unmixed components are light yellow, it turns light green on mixing, and changes again to a deep reddish-amber after the REQUIRED 100°C HIGH-TEMPERATURE CURE. It develops strong, tough, mechanically stable bonds to a wide variety of fiber optic and optical materials that includes most metals, ceramics, glass and many plastics. TRA-BOND FS443 has good impact and thermal shock resistance, and yields excellent low stress, pot-and-polish connections which do not piston during cycle tests. It is also resistant to water and weathering, vapors and gases, most petroleum products, and an extended range of organic and inorganic environments. Information provided by Tra-Con Inc.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
Mixed
Solids Content 100 %
100 %
Reactive Solids Content
Viscosity 120000 cP

@Temperature 25.0 °C
120000 cP

@Temperature 77.0 °F
Mixed (sp #4, 0.3 rpm)
Mechanical Properties Metric English Comments
Hardness, Shore D 90
90
15 min @ 100°C
Adhesive Bond Strength 17.2 MPa
2500 psi
Lap shear, alum to alum, 15 min @ 100°C
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 175 °C
347 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 115 °C
239 °F
Ultimate Tg
Electrical Properties Metric English Comments
Dielectric Strength 15.7 kV/mm
400 kV/in
Processing Properties Metric English Comments
Cure Time 15.0 min

@Temperature 100 °C
0.250 hour

@Temperature 212 °F
Pot Life 300 min
300 min
Descriptive Properties Value Comments
Color Red-Brown
Cured