Atom Adhesives AA-BOND 2123 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-BOND 2123 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-BOND 2123 is a versatile steel metal/epoxy adhesive formulation developed for modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required. AA-BOND 2123 is easy-to-use adhesive system contains no solvents and cures fairly rapidly at room temperature to a hard, low shrinkage solid, which bonds readily to steel, aluminum, and other metals, wood, concrete, glass, ceramics and many plastics. AA-BOND 2123 is tough and durable, resistant to water, mild acids and alkalis, salts and salt solutions, lubricating oils, petroleum solvents, gasoline, jet fuels, alcohol and many other organic and inorganic materials, While it may be attracted to a magnet, it is essentially an electrical insulator which can be readily drilled, cut, sawed and machined with regular metal working tools Typical repair applications: jigs, molds, dies, fixtures, plumbing, automotive, castings, aircraft, ships, marine, salvage.Appearance: Steel GreyCure Type: Heat cure or Room TemperatureBenefits:CastingJigsMoldsForming DiesPlubing RepairsTool and dies patchingAutomotive repairsIndustrial maintenance Mix Ratio by weight: 100:10/Resin:HardenerSubstrates: Most metals, ceramic, glass and plastics Typical Application: Modern industrial repair, casting and bonding applications where a steel-like or cast iron finish is required.Information provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 2.34 g/cc
2.34 g/cc
uncured
Solids Content 100 %
100 %
reactive, uncured
Viscosity 32000 cP
32000 cP
Mechanical Properties Metric English Comments
Hardness, Shore D 88
88
Thermal Properties Metric English Comments
CTE, linear 38.0 µm/m-°C
21.1 µin/in-°F
Thermal Conductivity 0.589 W/m-K
4.09 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 135 °C
275 °F
Minimum Service Temperature, Air -60.0 °C
-76.0 °F
Glass Transition Temp, Tg 110 °C
230 °F
Shrinkage 0.080 %
0.080 %
Processing Properties Metric English Comments
Cure Time 240 min

@Temperature 65.0 °C
4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 30.0 min
30.0 min
uncured
Descriptive Properties Value Comments
Thixotropic Index 1
Users viewing this material also viewed the following: