Thermal Properties | Metric | English | Comments |
---|---|---|---|
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon Silicone Hose and Duct Material with Polyester Substrate (65390R042)
(discontinued **) Side one - uncured silicone, 0.005 in., -0.001(0.1 mm, -0.01); Substrate - 6500 Polyester Fabric, 0.038 in. (0.97 mm) nominal; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.042 in.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.015" (0.381 mm) Semi-Cured Silicone Traction Motor Insulation with Fiberglass Substrate (51224R015)
&n 0.007 in. (0.18 mm) nominal semi-cured silicone rubber on 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass; 0.003 in. (0.8 mm) polyethylene interleave; overall thickness 0.015 in. ± 0.0015 (0.038 mm.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.008" (0.2032 mm) Thermabond® E-35 Uncured Silicone (99730N008) 0.008 in., ±0.001 (0.2 mm, ±0.03) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in ±0.001(0.2 mm ± 0.03). T.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.008" (0.2032 mm) Thermabond®-45 Uncured Silicone (99720W008) 0.008 in., +0.000,-0.002(0.2 mm, +0.00, -0.05) uncured silicone on 0.003 in. (0.08 mm) nominal PTFE coated fiberglass; 0.001 in. (0.03 mm) FEP interleave; overall thickness 0.008 in +0.000,-0.002(0... |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.010" (0.254 mm) Flexible Heater Silicone with Fiberglass Substrate (49586R010) Cured silicone rubber with a minimum thickness of 0.0015 in. (0.038 mm)/ 0.0055 in. (0.14 mm) Prime Coated 1681 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.003 in. (0.08 mm); 0... |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.010" (0.254 mm) Layer-on-Layer Silicone Traction Motor Insulation (51229R020) 0.010 in. (0.25 mm) minimum uncured silicone on 0.002 in. (0.5 mm) minimum cured silicone on 0.008 in. (0.2 mm) nominal Prime Coated 7628 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; ove.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.011" (0.2794 mm) Uncured Silicone Traction Motor Insulation (P29600R011) 0.006 in., +0.002, -0.001(0.2 mm, +0.05, -0.03) uncured silicone on 0.005 in. (0.08 mm) nominal PTFE coated fiberglass; 0.0015 in. (0.038 mm) polyethylene interleave; overall thickness 0.011 in ±0... |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51571R015) Cured silicone rubber with a minimum thickness of 0.0035 in. (0.08 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.0035 in. (0.1 mm); 0.003.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51576R015) Cured silicone rubber with a minimum thickness of 0.002 in. (0.05 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.005 in. (0.1 mm); 0.003 i.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51581R015) Uncured silicone rubber with a minimum thickness of 0.0035 in. (0.0889 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.0035 in. (0.0889 mm).. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51941C015) Uncured silicone rubber with a minimum thickness of 0.003 in. (0.08 mm)/0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.003 in. (0.08 mm); 0.003.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.015" (0.381 mm) Flexible Heater Silicone with Fiberglass Substrate (51946C015) Cured silicone rubber with a minimum thickness of 0.002 in. (0.05 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.005 in. (0.1 mm); 0.003 i.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.020" (0.508 mm) Flexible Heater Silicone with Fiberglass Substrate (51576R020) Cured silicone rubber with a minimum thickness of 0.003 in. (0.08 mm)/ 0.008 in. (0.2 mm) Prime Coated 7628 Fiberglass/Uncured silicone rubber with a minimum thickness of 0.009 in. (0.2 mm); 0.003 i.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.020" (0.508 mm) Layer-on-Layer Silicone Traction Motor Insulation (P29609R020) 0.010 in. (0.25 mm) minimum uncured silicone on 0.002 in. (0.5 mm) minimum cured silicone on 0.008 in. (0.2 mm) nominal Prime Coated 7628 Fiberglass; 0.0015 in. (0.038 mm) polyethylene interleave; o.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.020" (0.508 mm) Silicone Traction Motor Insulation with Fiberglass Substrate (19220R020) Uncured silicone rubber with a minimum thickness of 0.005 in. (0.13 mm) on Prime Coated 1523 Fiberglass; 0.0015 in. (0.8 mm) polyethylene interleave; overall thickness 0.020 in ± 0.0015 (0.51 mm ±.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.027" (0.6858 mm) Flexible Heater Silicone with Fiberglass Substrate (56586R028) Side one - uncured silicone, 0.003 in. (0.08 mm) minimum; Substrate - Prime Coated 162 Fiberglass, 0.019 in. (0.48 mm) nominal; Side two - cured silicone, 0.005 in. (0.1 mm) minimum; 0.003 in. (0.08.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.028" (0.7112 mm) Flexible Heater Silicone with Fiberglass Substrate (55586R028) 0.004 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.028" (0.7112 mm) Flexible Heater Silicone with Fiberglass Substrate (55586W028) 0.004 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579A028) 0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579GA028) 0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55579R028) 0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.029" (0.7366 mm) Flexible Heater Silicone with Fiberglass Substrate (55589R028) 0.005 in. (0.1 mm) minimum uncured silicone on 0.006 in. (0.2 mm) minimum cured silicone on 0.018 in. (0.46 mm) nominal Prime Coated 162 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; over.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.030" (0.762 mm) Silicone Traction Motor Insulation with Fiberglass Substrate (19220R030) Uncured silicone rubber with a minimum thickness of 0.015 in.(0.38 mm) on Prime Coated 1523 Fiberglass; 0.0015 in. (0.8 mm) polyethylene interleave; overall thickness 0.030 in ± 0.003 (0.76 mm ± 0.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon Thermavac® 0.020" (0.508 mm) Uncured Silicone Vacuum Bagging (30400R020) Uncured, unsupported silicone rubber with a thickness of 0.020 in ± 0.002 (0.51 mm ± 0.051) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.08 mm) polyethylene interleave.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon Thermavac® 0.030" (0.762 mm) Uncured Silicone Vacuum Bagging (30400N030) Uncured, unsupported silicone rubber with a thickness of 0.030 in ± 0.003 (0.76 mm ± 0.038) on a Kodacel carrier (0.005 in., 0.13 mm nominal thickness); 0.003 in. (0.8 mm) polyethylene interleave... |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon Thermavac® 0.040" (0.762 mm) Cured Silicone Vacuum Bagging (10502R040) Unsupported cured/post cured silicone rubber with a thickness of 0.040 in. ±0.004 (1.0 mm ±0.10); 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502N060) Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15 ); 0.003 in. (0.8 mm) polyethylene interleave. Color: Translucent. Weight: 2339 g/m² ± 234 (69.0.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon Thermavac® 0.060" (1.524 mm) Cured Silicone Vacuum Bagging (10502R060) Unsupported cured/post cured silicone rubber with a thickness of 0.060 in. ±0.006 (1.5 mm ±0.15); 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.008" (0.2032 mm) Flexible Heater Silicone with Fiberglass Substrate (44571R008) 0.0015 in. (0.038 mm) minimum Cured silicone rubber/Prime Coated 7628 Fiberglass/ 0.0015 in (0.038 mm) minimum uncured silicone rubber; 0.0015 in. (0.038 mm) polyethylene interleave; overall thickne.. |
|||
Minimum Service Temperature, Air | -56.6 °C | -69.9 °F | |
Arlon 0.008" (0.2032 mm) Flexible Heater Silicone with Fiberglass Substrate (49580R010) Uncured silicone rubber with a minimum thickness of 0.0045 in. (0.11 mm) on 0.0055 in. (0.14 mm) Prime Coated 1681 Fiberglass; 0.003 in. (0.08 mm) polyethylene interleave; overall thickness 0.010 in.. |