Material Notes:
Unsupported cured/post cured silicone rubber with a thickness of 0.040 in. ±0.004 (1.0 mm ±0.10); 0.003 in. (0.8 mm) polyethylene interleave. The shelf life is defined as the duration of time for which the product will meet the physical requirements outlined below. It does not guarantee the product’s usefulness in all applications. Color: Red. Weight: 1560 g/m² ± 67.8 (46.0 oz./yd.² ± 2.0). Shelf Life: 12 months from date of manufacture at 4.4°C (40°F).Applications: Composite vacuum bagging materials.Information provided by the manufacturer, Arlon Silicone Technologies Division.
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 60
50 - 60
Tensile Strength, Ultimate 7.47 - 9.13 MPa
1080 - 1320 psi
Elongation at Break 540 - 660 %
540 - 660 %
100% Modulus 0.00172 GPa
0.249 ksi
Average
Tear Strength >= 43.8 kN/m
>= 250 pli
Compression Set 28 %
28 %
after post cure
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.6 °C
-69.9 °F
Electrical Properties Metric English Comments
Dielectric Strength >= 15.75 kV/mm
>= 400.0 kV/in