Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Flame Retardant
Manufacturer Plastcom spol. s r.o.
Trade Name SLOVALEN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with the halogen flame retardant. Application - stadium seats with guaranteed life-cycle of the mechanical and surface properties, electrical industry - terminals, coil forms, covers of electrotools, guides. Fulfills 960°C glow wire and flammability in accordance with UL 94 V2. Concerning flammability, it complies with the building norm DIN 4102-B2. Delivered in the full RAL color scale.Application: Injection MouldingInformation Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 0.930 g/cc
0.0336 lb/in³
STN 64 0111
Linear Mold Shrinkage 0.0244 cm/cm
0.0244 in/in
STN 64 0808
Linear Mold Shrinkage, Transverse 0.0239 cm/cm
0.0239 in/in
STN 64 0808
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
STN EN ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 28.0 MPa
4060 psi
STN EN ISO 527-2
Elongation at Break 20 %
20 %
STN EN ISO 527-2
Tensile Modulus 1.20 GPa
174 ksi
STN EN ISO 527-2
Flexural Strength 35.0 MPa
5080 psi
STN EN ISO 178
Flexural Modulus 1.00 GPa
145 ksi
STN EN ISO 178
Charpy Impact Unnotched 11.0 J/cm²

@Temperature -20.0 °C
52.3 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
STN EN ISO 179
Charpy Impact, Notched 0.400 J/cm²

@Temperature -20.0 °C
1.90 ft-lb/in²

@Temperature -4.00 °F
STN EN ISO 179
0.900 J/cm²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
STN EN ISO 179
Thermal Properties Metric English Comments
Melting Point 150 °C
302 °F
DSC; STN EN ISO 3146
Deflection Temperature at 1.8 MPa (264 psi) 75.0 °C
167 °F
STN EN ISO 75/A
Vicat Softening Point 110 °C
230 °F
B; STN EN ISO 306
Flammability, UL94 V-2
V-2
Glow Wire Test 960 °C
1760 °F
STN IEC 60695-2-10
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
STN IEC 60093
Surface Resistance 1.00e+16 ohm
1.00e+16 ohm
STN IEC 60093
Dielectric Strength 24.0 kV/mm
610 kV/in
STN IEC 60243
Comparative Tracking Index 450 V
450 V
STN 34 6468
Processing Properties Metric English Comments
Melt Temperature 200 - 250 °C
392 - 482 °F
Mold Temperature 30.0 - 50.0 °C
86.0 - 122 °F
Injection Pressure 50.0 - 80.0 MPa
7250 - 11600 psi