Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 54.0 °C @Load 1.00 kg |
129 °F @Load 2.20 lb |
ISO 306/A |
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | 1kg load; ASTM D1525 |
Westlake EMAC® SP2209 Specialty Copolymer
(discontinued **) EMAC resins adhere to and are compatible with a wide range of materials including paper, polyolefins, oriented polyolefins, polyesters, ionomers, PVdC, unplasticized PVC and other polar polymers. Fo.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 8000 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | B (50N); ISO 306 |
Borealis Daplen™ EE137AI Polypropylene Compound 10% Mineral Filled Daplen EE137AI is a 10% mineral filled grade intended for injection molding. EE137AI has been developed especially for the car industry, to be used in interior parts where high scratch resistance i.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | A<sub>50</sub> (10N); ASTM D1525 - ISO 306 |
DuPont Elvaloy® 1820 AC Ethylene and 20% Methyl Acrylate Copolymer Elvaloy® 1820 AC is intended for film coextrusion, compounding and injection molding. Due to its high melt flow rate, it also can be used in extrusion coating/lamination. Elvaloy® 1820 AC has go.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525 |
DuPont Elvax® 3176 Ethylene-Vinyl Acetate Copolymer Resin for Coextrusion, Extrusion Coating 18 wt% Vinyl Acetate.Elvax® 3176 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525 |
Westlake EMAC® SP2252 20.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2252 is a 20.5% EMA copolymer containing slip and antiblock. This resin is designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal te.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525 |
DuPont Appeel® LSR20D745 Lidding Sealant Resin Appeel® LSR20D745 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad temperatu.. |
|||
Vicat Softening Point | 53.9 °C | 129 °F | ASTM D1525 |
ExxonMobil Escorene™ LD 723.28 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra UL 723.28 is a high VA extrusion coating resin, which provides outstanding heat sealability and high clarity. LD 723.28 has a good balance of drawabilty and neck-.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525, ISO 306 |
DuPont™ Appeel® 20D855 Ethylene Acrylate DuPont™ Appeel 20D855 is a modified ethylene acrylate resin designed to function as a sealing layer for lidding applications. It is most often suggested to provide peelable seals over a broad tempe.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525, ISO 306 |
DuPont™ Bynel® 22E757 Modified Ethylene Acrylate BYNEL® Series 2200 resins are modified ethylene acrylate resins. They contain a temperature stable ester which makes them functional in high temperature coextrusions. They are available in pellet f.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525, ISO 306 |
DuPont™ HPF® 2000 Amorphous Polymer for Golf Balls DuPont™ HPF 2000 offers high COR and lower compression. This combination of properties makes it extremely versatile and possible for this polymer to be used as a core, mantle, or cover in a golf ba.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525 |
Dow Engage® ENR 7270.00 Ethylene-Butene Copolymer Description: ENR 7270.00 is a general purpose ethylene-butene copolymer designed to provide good cost/performance balance in polymer modification applications.Information provided by manufacturer.Th.. |
|||
Vicat Softening Point | 54.0 - 56.0 °C | 129 - 133 °F | ISO R 306 |
Fainplast Compounds MRT 168 Medical Rigid PVC, Injection Molding Anti impact connectors |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525 |
Arkema Group OREVAC® 9318 EVA Terpolymer OREVAC® is a range of ethylene-vinyl acetate copolymers modified by adjunction of polar groups which, when molten, have excellent adhesive properties to various substrates. They are supplied as fre.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | |
BASF Novolen® 3520 L Polypropylene Grade containing antiblocking agent; sealing layer for OPP film.Data was collected by ISO methods and provided by BASF. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525, ISO 306 |
DuPont Elvax® 3176CW-3 Ethylene Vinyl Acetate
(discontinued **) DuPont™ Elvax® 3176CW-3 is an extrudable ethylene-vinyl acetate copolymer resin available in pellet form for use in conventional extrusion equipment designed to process polyethylene resins. Additi.. |
|||
Vicat Softening Point | 54.0 - 165 °C | 129 - 329 °F | Average value: 119 °C Grade Count:71 |
Overview of materials for Polypropylene with 40% Talc Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 40% Talc Filler". Specific grades with primary filler content between 35% and 44% are.. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | Rate B; ASTM D-1525 |
ExxonMobil Iotek® 8020 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A sodium ionomer with excellent abrasion resistance, impact strength, hardness and tensile strength. IOTEK ionomers provide superb low temperature .. |
|||
Vicat Softening Point | 54.0 °C | 129 °F | ASTM D1525 |
DuPont Appeel® LSR 2044 Modified EVA Lidding Sealing Resin Appeel® 2044 is a blown or cast film resin designed to be a sealing layer for lidding applications. It provides a peelable seal over a broad temperature range to a number of container materials inc.. |