Fainplast Compounds MRT 168 Medical Rigid PVC, Injection Molding

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Rigid Grade
Manufacturer Fainplast Compounds
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Fainplast Compounds MRT 168 Medical Rigid PVC, Injection Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Anti impact connectors
Physical Properties Metric English Comments
Density 1.29 - 1.33 g/cc
0.0466 - 0.0480 lb/in³
ISO R 1183
Mechanical Properties Metric English Comments
Tensile Strength at Break 33.0 MPa
4790 psi
ISO R 527
Tensile Strength, Yield 35.0 MPa
5080 psi
ISO R 527
Elongation at Break 230 %
230 %
ISO R 527
Thermal Properties Metric English Comments
Vicat Softening Point 54.0 - 56.0 °C
129 - 133 °F
ISO R 306
Descriptive Properties Value Comments
Properties according to Pharmacopoeia 4th edition NO