Mechanical Properties Metric English Comments
Flexural Strength 170 MPa

@Temperature 125 °C
24700 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 150FW30 PEEK, 30% Carbon Fibre/PTFE Reinforced
Product Description:High performance thermoplastic material, 30% reinforced with carbon fibre / PTFE Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA fo..
Flexural Strength 170 MPa

@Temperature 23.0 °C
24700 psi

@Temperature 73.4 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-400G15 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 170 MPa

@Temperature -40.0 °C
24700 psi

@Temperature -40.0 °F
Practical Use (Water Absorption 2.1%); ASTM-D790
Toyobo GLAMIDE® T-663G15 Nylon-66
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 170 MPa

@Temperature -40.0 °C
24700 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® T-777-02 Nylon-6
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 170 MPa

@Temperature -40.0 °C
24700 psi

@Temperature -40.0 °F
Absolute Drying; ASTM-D790
Toyobo GLAMIDE® NB-5550 Nylon/Olefin
GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a..
Flexural Strength 170 MPa

@Treatment Temp. 100 °C,
Time 3600 sec
24700 psi

@Treatment Temp. 212 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m..
Flexural Strength 170 MPa

@Thickness >=1.50 mm
24700 psi

@Thickness >=0.0591 in
24hr/23°C/50% RH; ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..
Flexural Strength 170 MPa

@Treatment Temp. 20.0 °C,
Time 3600 sec
24700 psi

@Treatment Temp. 68.0 °F,
Time 1.00 hour
ISO 178; IEC/EN 60893-2 5.1
Elektro-Isola G-Etronax PM GPO 3 Polyester, Glass Mat, Red, Sheets
Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free.Applica..
Flexural Strength >= 170 MPa

@Temperature 150 °C
>= 24700 psi

@Temperature 302 °F
Perpendicular to laminations; IEC 1212-2 5.1
Hippe EP GC 203 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Flexural Strength >= 170 MPa

@Temperature 150 °C
>= 24700 psi

@Temperature 302 °F
Perpendicular to laminations; IEC 1212-2 5.1
Hippe EP GC 204 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Flexural Strength >= 170 MPa

@Temperature 150 °C
>= 24700 psi

@Temperature 302 °F
Perpendicular to laminations; IEC 1212-2 5.1
Hippe EP GC 205 Woven Glass Cloth Reinforced Epoxy Resin - Sheet
Used in mechanical, electrical and electronic applications. Extremely high mechanical strength at moderate temperature. Very good stability of electrical properties under high humidity. High mech..
Flexural Strength 170 MPa

@Temperature -40.0 °C
24700 psi

@Temperature -40.0 °F
ASTM D790
BASF Ultramid® 8202 L Intermediate PA6 (Dry)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
Flexural Strength 170 MPa

@Temperature -40.0 °C
24700 psi

@Temperature -40.0 °F
ISO 178
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT  (Unverified Data**)
Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis..
Flexural Strength 170 MPa

@Temperature 125 °C
24700 psi

@Temperature 257 °F
ISO 178
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical..