Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 90.0 MPa @Temperature 125 °C |
13100 psi @Temperature 257 °F |
ISO 178 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 90.0 MPa @Temperature 125 °C |
13100 psi @Temperature 257 °F |
ISO 178 |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |
|||
Flexural Strength | 90.0 MPa @Temperature 275 °C |
13100 psi @Temperature 527 °F |
ISO 178 |
Victrex® PEEK 450CA40 Polyetheretherketone, 40% Carbon Fibre Reinforced Product Description:High performance thermoplastic material, 40% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Flexural Strength | 90.0 MPa @Temperature 125 °C |
13100 psi @Temperature 257 °F |
ISO 178 |
Victrex® PEEK 90G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Flexural Strength | 90.0 MPa @Strain 3.50 % |
13100 psi @Strain 3.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Flexural Strength | 90.0 MPa @Strain 3.50 % |
13100 psi @Strain 3.50 % |
d.a.m., 2 mm/min; ISO 178-A |
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity PA 6, non-reinforced, extrusion, low viscosity, no additivesInformation provided by LANXESS. |
|||
Flexural Strength | 90.0 MPa @Temperature 23.0 °C |
13100 psi @Temperature 73.4 °F |
Practical Use; ASTM-D790 |
Toyobo GLAMIDE® TY-835TC Nylon-66 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 90.0 MPa @Temperature 23.0 °C |
13100 psi @Temperature 73.4 °F |
Absolute Drying; ASTM-D790 |
Toyobo GLAMIDE® T-422VOR Nylon-6 GLAMIDE® is very tough and exhibits high abrasion resistance. It has a high melting point and heat resistance, has well-balanced proportions of mechanical properties, performs self-distinguishing a.. |
|||
Flexural Strength | 90.0 MPa @Treatment Temp. 150 °C, Time 3600 sec |
13100 psi @Treatment Temp. 302 °F, Time 1.00 hour |
ISO 178; IEC/EN 60893-2 5.1 |
Elektro-Isola G-Etronax PM 953 Polyester, Glass Mat, Off White, Sheets Description: Good electrical properties such as high breakdown voltage in air and oil and highest arc resistance and tracking resistance. Self-extinguishing. Low smoke emission, halogen-free. Very m.. |
|||
Flexural Strength | 90.4 MPa @Temperature 23.0 °C |
13100 psi @Temperature 73.4 °F |
ASTM D790 |
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts Higher abrasion resistance than G15, high value stability and very low friction coefficient propertyInformation provided by Daelim H&L |