Dow Corning HV 1760/80 SILICONE RUBBER NATURAL

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone , Silicone Rubber
Manufacturer Dow Corning
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning HV 1760/80 SILICONE RUBBER NATURAL.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
80 Shore hardness high consistency silicone rubber with fast cure system and excellent tracking and erosion resistanceInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.53 g/cc

@Temperature 25.0 °C
1.53 g/cc

@Temperature 77.0 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 79
79
Tensile Strength, Ultimate 4.83 MPa
700 psi
Elongation at Break 150 %
150 %
Tear Strength 16.0 kN/m
91.0 pli
Electrical Properties Metric English Comments
Volume Resistivity 5.40e+14 ohm-cm
5.40e+14 ohm-cm
Dielectric Constant 3.61

@Frequency 100 Hz
3.61

@Frequency 100 Hz
Dielectric Strength 17.0 kV/mm
433 kV/in
Processing Properties Metric English Comments
Shelf Life 3.00 Month
3.00 Month
Descriptive Properties Value Comments
Color grey
Hydrophobic yes