Parker Chomerics CHO-SEAL S6304 Conductive Elastomer

Category Polymer , Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL S6304 Conductive Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Conductive Elastomer EMI/EMP GasketsInformation provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.65 - 2.15 g/cc
1.65 - 2.15 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 45 - 65
45 - 65
Tensile Strength at Break >= 1.03 MPa
>= 150 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Tear Strength 6.13 kN/m
35.0 pli
Compression Set 30 %
30 %
70 hrs @ 100°C; ASTM D395 Method B
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -45.0 °C
-49.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 0.10 ohm-cm
0.10 ohm-cm
as supplied without pressure sensitive adhesive
Shielding Effectiveness >= 100 dB
>= 100 dB
2 GHz (Plane Wave); MIL-G-83528
>= 100 dB
>= 100 dB
10 GHz (Plane Wave); MIL-G-83528
>= 100 dB
>= 100 dB
100 MHz (E Field); MIL-G-83528
>= 100 dB
>= 100 dB
500 MHz (E Field); MIL-G-83528
Descriptive Properties Value Comments
Binder Silicone
EMP Survivability kA / in, min 0.1
Filler Ni/C
Heat Aging ohm-cm max 0.25