Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Rubber or Thermoset Elastomer (TSE) , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-SEAL®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-SEAL® 6315 Graphite Filled Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EMI Gaskets. This extruded nickel-plated graphite filled elastomer addresses EMI shielding and environmental needs for both internal and external applications. It has an excellent performance in salt spray corrosion applications and there are options for addressing fluid immersion requirements as well as Underwriters Laboratories flammability requirements.Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.55 - 2.05 g/cc
1.55 - 2.05 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore A 50 - 64
50 - 64
Tensile Strength at Break >= 0.965 MPa
>= 140 psi
Elongation at Break >= 100 %
>= 100 %
Tear Strength 6.13 kN/m
35.0 pli
Compression Set 30 %
30 %
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -40.0 °C
-40.0 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Volume Resistivity <= 750 ohm-cm
<= 750 ohm-cm
initial; CEPS-0002
<= 850 ohm-cm
<= 850 ohm-cm
Aged; CEPS-0002
Shielding Effectiveness >= 80 dB
>= 80 dB
500 MHz (E Field); MIL-G-83528
>= 80 dB
>= 80 dB
2 GHz (Plane Wave); MIL-G-83528
>= 80 dB
>= 80 dB
10 GHz (Plane Wave); MIL-G-83528
>= 80 dB
>= 80 dB
100 MHz (E Field); MIL-G-83528
Descriptive Properties Value Comments
Binder Silicone
Filler Ni/C
Galvanic Corrosion - CHO TM-100 mg 35