Polymer Property : Tear Strength = 40.0 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength >= 40.0 kN/m
>= 228 pli
ASTM D624
Multibase Multi-Flex® TPE G 7455 S BLK
The burn rate is 0 in/min (0 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 40.0 kN/m
228 pli
Die B,post cured- 2 hours at 200°C; ASTM D624
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tear Strength 40.0 kN/m
228 pli
as molded; Die B
Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer
Information provided by Multibase
Tear Strength 40.0 kN/m
228 pli
ISO 34-1
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE)
OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu..
Tear Strength 40.0 kN/m
228 pli
ISO 34B
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane
AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh..
Tear Strength 40.0 kN/m
228 pli
ISO 34B
Huntsman AVALON® 65 AK-ESD Thermoplastic Polyurethane
AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh..
Tear Strength 40.0 kN/m
228 pli
DIN 53515
Kraiburg TPE THERMOLAST® K TA8HAI Injection Molding TPE
Compound easy printable, paintable, glueable without pretreatmentColorable in any shadeSubstitution for PVC and silicone rubberTypical Applications: ToysBaby productsPromotion articlesMaterial Advan..
Tear Strength 40.0 kN/m
228 pli
DIN 53515
Kraiburg TPE THERMOLAST® K TC9CHT Transparent Extrusion TPE
Transparent compound for extrusionSubstitute for silicon and PVC-PExtremely flexible materialColoring in any shadeTypical Applications: Design (e.g. grip elements and functional elements for furnitu..
Tear Strength 40.0 kN/m
228 pli
MD; ISO 6383-2
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene
LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co.
Tear Strength 40.0 kN/m
228 pli
Die B
Momentive Performance Materials Siloprenâ„¢ Electro 242-3 Electrically Insulating Liquid Silicone Rubber
This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
Tear Strength 40.0 kN/m
228 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 2345/06 Electrically-Conductive Liquid Silicone Rubber
This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate..
Tear Strength 40.0 kN/m
228 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 3285/50 Liquid Silicone Rubber - Self-Lubricating / Standard
This LSR elastomer is a self-lubricating, standard, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at eleva..
Tear Strength 40.0 kN/m
228 pli
Die B
Momentive Performance Materials Siloprenâ„¢ LSR 3286/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set
This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time..
Tear Strength >= 40.0 kN/m
>= 228 pli
DIN 53507
Karina CAK 75-48/1 Black PVC Compound
Reclaimed PVC compound recommended for soles injectionInformation provided by Karina Indústria e Comércio de Plásticos Ltda.
Tear Strength >= 40.0 kN/m
>= 228 pli
DIN 53507
Karina 70/222 Clear PVC Compound
Information provided by Karina Indústria e Comércio de Plásticos Ltda.
Tear Strength 40.0 kN/m
228 pli
Shin-Etsu Silicones LIMSâ„¢ KEG2001-50A/B Elastomer
KEG2001-50 is a very fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enou..
Tear Strength 40.0 kN/m
228 pli
DIN 53515
Lubrizol ESTANE® T5275 Ether Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 40.0 kN/m
228 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.25 PHR Zinc Stearate
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 40.0 kN/m
228 pli
Trelleborg R698 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 40.0 kN/m
228 pli
Trelleborg R798 Commercial Natural Rubber Polyisoprene
All information provided by Trelleborg
Tear Strength 40.0 kN/m
228 pli
DIN 53515
Lubrizol ESTANE® 54660 Ester Based Thermoplastic Polyurethane (European Grade)
Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability ..
Tear Strength 40.0 kN/m
228 pli
ISO 34
Chengdu Polyster CH4132 Thermoplastic Polyether-ester Elastomer (TPEE)
Poly-basic block copolymer. Good compatibility with POM. For blending with POM to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd.
Tear Strength 40.0 kN/m
228 pli
ASTM D624
ELASTO UK Dryflex® 500800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Translucent
The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha..
Tear Strength 40.0 kN/m
228 pli
Die C; ASTM D624
Covestro Bayflex® MP-10000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System
0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of..
Tear Strength 40.0 kN/m
228 pli
DIN ISO 34-1/Bb
BASF Elastollan S 50 A SPF TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat..
Tear Strength 40.0 kN/m
228 pli
Die C; ASTM D412
Alliance Polymers Zythane™ 5070A Thermoplastic Polyurethane Elastomer
Zythane™ 5070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good ..
Tear Strength 40.0 kN/m
228 pli
ISO 34-1
Celanese RITEFLEX XFR 440 TPC, Unfilled
Riteflex XFR 440 is a nominal 40 Shore D thermoplastic polyester elastomer featuring a halogen-free flame retardant system. It is UL certified to be V-0 at 1.5 mm in all colors. It exhibits an excel..
Tear Strength >= 40.0 kN/m
>= 228 pli
ISO 34
Austin Novel Materials Texalan® 365A Polyester-based TPU
Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech
Tear Strength 40.0 kN/m
228 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.25 PHR Zinc Stearate
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 40.0 kN/m
228 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Thanecure® ZM
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..