Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Low Density Polyethylene (LDPE), Film Grade
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) LS0085/KJ Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LS0085/KJ is a high molecular weight low density polyethylene film grade combining good flexible extrusion behavior and superior mechanical properties.Application: shrink packaging.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.921 g/cc
0.0333 lb/in³
ISO 1183
Melt Flow 0.85 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.85 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ISO 527
Film Tensile Strength at Yield, TD 11.0 MPa
1600 psi
ISO 527
Elongation at Break 200 %
200 %
ISO 527, MD
500 %
500 %
ISO 527, TD
Modulus of Elasticity 0.160 GPa
23.2 ksi
MD; ISO 527
0.170 GPa
24.7 ksi
TD; ISO 527
Tensile Impact 300 J/cm
562 ft-lb/in
ASTM D4272
Coefficient of Friction 0.10
0.10
ASTM D1894
Tear Strength 30.0 kN/m
171 pli
TD; ISO 6383-2
40.0 kN/m
228 pli
MD; ISO 6383-2
Optical Properties Metric English Comments
Haze 12 %
12 %
ASTM D1003A
Gloss 49 %
49 %
ASTM D2457
Descriptive Properties Value Comments
Clarity, mV 37
Sabtec