Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 40.0 - 362 kN/m | 228 - 2070 pli | Average value: 137 kN/m Grade Count:115 |
Overview of materials for Polyester Thermoplastic Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyester Thermoplastic Elastomer". Each property range of values reported is minimum and maximum values.. |