Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer

Category Polymer , Thermoset , Silicone
Manufacturer Multibase
Trade Name SILASTIC®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase SILASTIC® C7-4565 CADOX BSD Dow-Corning Biomedical Grade ETR Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Multibase
Mechanical Properties Metric English Comments
Hardness, Shore A 46
46
post cured- 4 hours at 204°C
61
61
as molded
66
66
post cured- 2 hours at 177°C
Tensile Strength, Ultimate 7.93 MPa
1150 psi
post cured- 4 hours at 204°C
7.943 MPa
1152 psi
post cured- 2 hours at 177°C
8.219 MPa
1192 psi
as molded
Tensile Strength, Yield 3.52 MPa
511 psi
at 200%, as molded
4.41 MPa
640 psi
at 200%, post cured- 2 hours at 177°C
4.65 MPa
675 psi
200%, post cured- 4 hours at 204°C
Elongation at Break 411 %
411 %
post cured- 4 hours at 204°C
448 %
448 %
post cured- 2 hours at 177°C
547 %
547 %
as molded
Tear Strength 28.6 kN/m
163 pli
post cured- 2 hours at 177°C; Die B
30.7 kN/m
175 pli
post cured- 4 hours at 204°C; Die B
40.0 kN/m
228 pli
as molded; Die B
Users viewing this material also viewed the following: