Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 40.0 kN/m | >= 228 pli | Method B; ISO 34 |
S&E Specialty Polymers SE900-6 PVC Description: PVC weatherable, integral colored, filledApplications: Roof Ditch Molding Skin which meets the Ford WSKM4D689-A5Information provided by S&E Specialty Polymers |
|||
Tear Strength | 39.9 kN/m | 228 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ISO 34B |
Huntsman AVALON® 60 AE-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ISO 34B |
Huntsman AVALON® 65 AK-ESD Thermoplastic Polyurethane AVALON® ESD range are soft TPUs that deliver the improved bonding strength and mechanical properties required to produce high-quality footwear on roundtable machines – specifically safety sh.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | MD; ISO 6383-2 |
Iran Petrochemical (PCC) 2101TN47 Low Density Polyethylene LDPE 2101TN47 Shrink FilmThis grade enables high speed production of film without blocking.Information provided by Iran Petrochemical Commercial Co. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ Electro 242-3 Electrically Insulating Liquid Silicone Rubber This LSR elastomer is an electrically insulating, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 2345/06 Electrically-Conductive Liquid Silicone Rubber This LSR elastomer is an electrically conductive, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle times, at elevate.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials Siloprenâ„¢ LSR 3486/50 Liquid Silicone Rubber - Self-Lubricating / Low Compression Set This LSR elastomer is a self-lubricating, low compression set, two-component, platinum (addition/heat) curable, and pumpable silicone elastomer that can be molded and cured with very fast cycle time.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die B |
Momentive Performance Materials TUFELâ„¢ II 94405 Low Volatile Extrusion Heat Cured Rubber Heat cured rubber is a high consistency product that can be molded, extruded or calendered using conventional rubber processing equipment to meet a wide range of cost, durability and performance sta.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | |
Shin-Etsu Silicones LIMSâ„¢ KEG2001-50A/B Elastomer KEG2001-50 is a very fast cure type liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enou.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | |
Shin-Etsu Silicones LIMSâ„¢ KE1950-70A/B Elastomer KE-1950-70 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. It's viscosity is low enough to allow easy .. |
|||
Tear Strength | 40.0 kN/m | 228 pli | |
Shin-Etsu Silicones LIMSâ„¢ KEG2000-50A/B Elastomer KEG2000-50 is a liquid injection molding silicone. It is supplied as two components which are mixed in a 1:1 ratio to ensure easy and accurate blending. Its viscosity is low enough to allow easy pum.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ASTM D624 |
Teknor Apex Monprene® MP-2860M Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN 53515 |
Lubrizol ESTANE® T5384 Ether Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Tear Strength | 39.9 kN/m | 228 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 0.0 PHR MBT MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 39.9 kN/m | 228 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 20 PHR N330 (HAF) Filler MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | GB/T 529 |
Chengdu Polyster 6500 General Grade TPV Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ISO 34 |
Chengdu Polyster CH4132 Thermoplastic Polyether-ester Elastomer (TPEE) Poly-basic block copolymer. Good compatibility with POM. For blending with POM to improve impact resilience properties.Information provided by Chengdu Polyster Co., Ltd. |
|||
Tear Strength | 40.0 kN/m | 228 pli | ASTM D624 |
ELASTO UK Dryflex® 500800S SEBS Based Material, Unfilled Qualities, 80A Hardness, Translucent The 500-seriesis very favorable when transparency and good scratch resistance are required, as well as when there are high surface finish requirements. Unfilled grades have excellent flow and mecha.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C; ASTM D624 |
Covestro Bayflex® MP-10000 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.118 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN ISO 34-1/Bb |
BASF Elastollan B 60 A ESD TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tensile strength, good damping and resilience performance and sup.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN ISO 34-1/Bb |
BASF Elastollan S 50 A SPF TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with excellent mechanical properties and wear resistance, good damping characteristics and a high resilience performance.Typical Applicat.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | DIN ISO 34-1/Bb |
BASF Elastollan SP 9213 TPUR Description: Thermoplastic Polyurethane Elastomers with excellent mechanical properties, outstanding wear resistance, high tear and tensile strength, good damping characteristics and a high resilien.. |
|||
Tear Strength | 40.0 - 280 kN/m | 228 - 1600 pli | Average value: 126 kN/m Grade Count:30 |
Overview of materials for Polyether Ester Elastomer This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr.. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C; ASTM D412 |
Alliance Polymers Zythane™ 4070A Thermoplastic Polyurethane Elastomer Zythane™ 4070A is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tear Strength | 40.0 kN/m | 228 pli | Die C |
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 0.5 PHR Thanecure® ZM MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st.. |