Polymer Property : Tear Strength = 242 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tear Strength 42.4 kN/m
242 pli
ASTM D624
Multibase Multi-Flex® TPE G 7410 NAT
The following properties were obtained from the Shell Kraton G 7410 and the Multibase 7410 products. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 42.4 kN/m
242 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 42.4 kN/m
242 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with DOP Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 42.4 kN/m
242 pli
Die B, post cured- 8 hours at 177°C; ASTM D624
Multibase C6-350 LH Parts A and B Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 42.4 kN/m
242 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with DOP Plasticizer
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 42.4 kN/m
242 pli
Die C
TSE Industries Millathane® HT High Temperature-Resistant Millable Polyester Polyurethane with 20 PHR N774 (SRF) Filler
MILLATHANE HT is a polyester millable polyurethane which has the ability to withstand elevated temperatures. Polyurethanes have been known for their excellent resistance to abrasion, impact, tear st..
Tear Strength 42.4 kN/m
242 pli
Dow Corning S50 LIQUID SILICONE RUBBER KIT
A heat-cured elastomer for use by customers fabricating medical devices, including those intended for implantation in humans for less than 30 days and non-implant applications. Dow Corning® S50 Liq..
Tear Strength 42.4 kN/m
242 pli
Die C; ASTM D 624
CPT C-Flex® R70-091 Opaque Biocompatible TPE
C-Flex® is a family of patented thermoplastic elastomers which range in hardness from 5 shore A to 95 shore A. C-Flex® TPE's are biocompatible polymer blends which meet or exceed the current..
Tear Strength 42.4 kN/m
242 pli
Dow Corning SILASTIC® LS 5-8760 FLUOROSILICONE RUBBER
60 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning
Tear Strength 42.4 kN/m
242 pli
Die 'C' Tear; 20 in/min; ASTM D624
PolyOne Elastamax XL 1092-35 TPU-Based Thermoplastic Elastomer  (discontinued **)
This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged..