Material Notes:
This is a general purpose thermoplastic elastomer based on modified TPU technology. Physical Form: Pellet. Standard Color: Natural.Information provided by M. A. Hanna. M. A. Hanna and Geon merged to form PolyOne in 2000.
Physical Properties Metric English Comments
Density 0.970 g/cc
0.0350 lb/in³
ASTM D792
Melt Flow 68 g/10 min

@Load 3.80 kg,
Temperature 190 °C
68 g/10 min

@Load 8.38 lb,
Temperature 374 °F
ASTM D1238
271.4 g/10 min

@Load 8.70 kg,
Temperature 190 °C
271.4 g/10 min

@Load 19.2 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 54
54
5 sec. delay; ASTM D2240
Tensile Strength, Ultimate 11.2 MPa
1620 psi
10 in/min; ASTM D412
Elongation at Break 716 %
716 %
10 in/min; ASTM D412
50% Modulus 0.00128 GPa
0.186 ksi
10 in/min; ASTM D412
100% Modulus 0.00168 GPa
0.244 ksi
ISO 37
200% Modulus 0.00217 GPa
0.315 ksi
10 in/min; ASTM D412
300% Modulus 0.00275 GPa
0.399 ksi
10 in/min; ASTM D412
Tear Strength 42.4 kN/m
242 pli
Die 'C' Tear; 20 in/min; ASTM D624
Tensile Set 10.8 %
10.8 %
at 100%; ASTM D412