Multibase Multi-Flex® TPE G 7410 NAT

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE G 7410 NAT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The following properties were obtained from the Shell Kraton G 7410 and the Multibase 7410 products. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 2.0 g/10 min
2.0 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 66
66
10 sec; ASTM D-2240
Tensile Strength, Ultimate 10.7 MPa
1550 psi
ASTM D412
Elongation at Break 690 %
690 %
ASTM D412
Tear Strength 42.4 kN/m
242 pli
ASTM D624