Mechanical Properties Metric English Comments
Tear Strength 24.5 kN/m
140 pli
ASTM D624
Multibase Multi-Flex® TPE A 6821 NAT
This product is based on Kraton G and PP. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength >= 24.5 kN/m
>= 140 pli
ASTM D624
Multibase Multi-Flex® TPE A 7606 BLK
The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Tear Strength 24.5 kN/m
140 pli
Die B, no post cure- press cured for 5 minutes; ASTM D624
Multibase SILASTIC® 7-6830 Dow-Corning Biomedical Grade Liquid Silicone Rubber
Information provided by Multibase
Tear Strength 24.5 kN/m
140 pli
ASTM D412
Multibase TPSiV™ 3010-50A Thermoplastic Silicone Vulcanizate
These materials are a novel family of TPV products based on cross-linked silicone rubber dispersed into various engineering thermoplastics. The dispersion of the silicone internal phase is produced..
Tear Strength 24.5 kN/m
140 pli
ASTM D624
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE)
Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established...
Tear Strength 24.5 kN/m
140 pli
ASTM D624
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,..
Tear Strength 24.5 kN/m
140 pli
ASTM D624
PolyOne Dynaflex™ G7960-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7960-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen..
Tear Strength 24.5 kN/m
140 pli
Certified
NuSil MED-4720 Two-Part Standard High Consistency Elastomers - Unrestricted Medical Use
Description: High consistency rubber, or HCR, consists of high molecular weight polymer combined with silica to produce a material that can be molded, extruded, or calendared into a useful end produ..
Tear Strength 24.5 kN/m
140 pli
Typical
NuSil MED-4725 Two-Part Standard High Consistency Elastomers - Unrestricted Medical Use
Description: High consistency rubber, or HCR, consists of high molecular weight polymer combined with silica to produce a material that can be molded, extruded, or calendared into a useful end produ..
Tear Strength 24.5 kN/m
140 pli
die C; ASTM D624
PB1100-55 Polyurethane-based Biomedical Elastomer
Tear Strength 24.5 kN/m
140 pli
Typical
NuSil MED-4120 Silicone, One Part High Consistent Elastomer - Restricted Medical Use
Description: HCRs can be used for extrusion of tubing and profiles (rod or ribbon), in calendared sheeting for die-cutting, or in compression or transfer molded parts such as balloons, gaskets or o-..
Tear Strength 24.5 kN/m
140 pli
DIN ISO 34-1
Kraiburg TPE For-Tec E OC6OAZ Thermoplastic Elastomer, Adhesion to PA
The AD/PAX/MR Series is recommended for two-component-seals in electronic applications and soft touch grips and handles of machine tools. The material provides an excellent resistance to skin oils, ..
Tear Strength 24.5 kN/m
140 pli
DIN ISO 34-1
Kraiburg TPE THERMOLAST® K TF7THT Thermoplastic Elastomer, high transparency
The FC/ht Series is a highly transparent material solution for applications with food contact. The series is characterized, among other things, by its excellent adhesion to PP. Typical applications:..
Tear Strength 24.5 kN/m
140 pli
DIN ISO 34-1
Kraiburg TPE THERMOLAST® K TP8VCN Thermoplastic Elastomer, Adhesion to PC, ABS, PETG, optimized compression set
The AD1/CS Series is recommended for applications with excellent adhesion to polar thermoplastics such as ABS, PC and PC/ABS as well as excellent compression set. The compounds are available in natu..
Tear Strength 24.5 kN/m
140 pli
Die B, post cured- 8 hours at 177°C; ASTM D624
Multibase C6-235 DI-CUP R Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 24.5 kN/m
140 pli
Die B, post cured- 8 hours at 177°C; ASTM D624
Multibase C6-250 PERKADOX PD-50S Dow-Corning Class VI Elastomer
Information provided by Multibase
Tear Strength 24.5 kN/m
140 pli
ASTM D624
Multibase Multi-Flex® A 8030 C2 Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase
Tear Strength 24.5 kN/m
140 pli
ASTM D624
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer
Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase
Tear Strength 24.5 kN/m
140 pli
Die C; ASTM D624
Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tear Strength 24.5 kN/m
140 pli
ASTM D624
Teknor Apex UNIPRENE® 7010-64 Thermoplastic Elastomer
Information provided by Teknor Apex Company
Tear Strength 24.5 kN/m
140 pli
Cytec EN-11 (Conap) Casting, Potting, and Molding Compound
High Technology Potting, Casting and Molding CompoundsTwo-component, polybutadiene-based liquid urethane casting and potting systems. When reacted these high technology systems produce tough, stable..
Tear Strength 24.5 kN/m
140 pli
at 25°C
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by..
Tear Strength 24.5 kN/m
140 pli
Die C, Vulcanizate, Press cured, TC95 +3min at 160°C
Dow Nordel® IP 4570 General Purpose Compound
FormulationNordel® IP 4570
Tear Strength 24.5 kN/m
140 pli
Warp, Breaking Strength w/o Sizing
3M Nextel™ AF-11 Aerospace Woven Fabric 312
Information provided by 3M
Tear Strength 24.5 kN/m
140 pli
Fill, Breaking Strength w/o Sizing
3M Nextel™ AF-11 Aerospace Woven Fabric 312
Information provided by 3M
Tear Strength 24.5 kN/m
140 pli
Die C (graves), 20 in/min; ASTM D624
PolyOne Synprene® IT 36-021 NATURAL Thermoplastic Elastomer - SBC  (discontinued **)
Description/Features:Specialty Thermoplastic ElastomerApplications: FDA (Food Contact)Processing Method: Injection MoldingInformation provided by PolyOne Corporation
Tear Strength 24.5 kN/m
140 pli
die B; ASTM D624
G-2706 Styrene-based Biomedical Elastomer
Tear Strength 24.5 kN/m
140 pli
die B; ASTM D624
G-2712 Styrene-based Biomedical Elastomer
Tear Strength 24.5 kN/m
140 pli
Trouser; ASTM D470
Lubrizol ESTANE® 58325 Ether Based Thermoplastic Polyurethane
Features: High melt strength for thick sheet extrusion.Uses: Blown and Flat Die/Cast Extrusion, Tubing and Profile ExtrusionAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformat..