Multibase Multi-Flex® TPE RP 6568 C340 BLK

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Multibase
Trade Name Multi-Flex® TPE
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Multibase Multi-Flex® TPE RP 6568 C340 BLK.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This product was designed for 2 shot airbag covers with lower tensile strength than currently in use. Ash is 2.2%. The moisture content is 0.05%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase.
Physical Properties Metric English Comments
Density 0.918 g/cc
0.0332 lb/in³
ASTM D792
Melt Flow 18 g/10 min
18 g/10 min
(Condition L) ASTM D-1238
Mechanical Properties Metric English Comments
Hardness, Shore A 56
56
10 sec; ASTM D-2240
Tensile Strength, Ultimate 2.90 MPa
421 psi
20"/min.; ASTM D-412
Elongation at Break 820 %
820 %
ASTM D638
Tear Strength 24.5 kN/m
140 pli
ASTM D624