Mechanical Properties Metric English Comments
Tear Strength 24.5 - 26.5 kN/m
140 - 151 pli
ASTM D624
Proto3000 Objet Digital Materials™ DM_9885/9785 Rubber-like Prototyping Polymer
Primary material: TangoBlackPlus/TangoPlusSecondary material: VeroWhitePlusDigital Materials are made up of two Objet materials. The two materials are combined in specific concentrations and structu..