Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | >= 24.5 kN/m | >= 140 pli | ASTM D624 |
Multibase Multi-Flex® TPE A 7606 BLK The burn rate is 1.2 in/min (30 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE) Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Versaflex™ OM 9-802CL Thermoplastic Elastomer (TPE) Versaflex™ OM 9-802CL is a clear, soft touch TPE designed to bond to the following thermoplastics: PC, ABS, PC/ABS and copolyester. New Product. Commercial specifications have not been established... |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
PolyOne Dynaflex™ G7960-1 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7960-1 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | die C; ASTM D624 |
PB1100-55 Polyurethane-based Biomedical Elastomer |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die B, post cured- 8 hours at 177°C; ASTM D624 |
Multibase C6-250 DI-CUP R Dow-Corning Class VI Elastomer Information provided by Multibase |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Multibase Multi-Flex® D 4003 Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection MoldingExtrusion Information provided by Multibase |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7370-1000 TPE Product Description: StarFlex P 7370-1000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelExcellent ColorabilityGood WeatherabilityFDA and medical grades avai.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C; ASTM D624 |
Teknor Apex APEX® 3055-H Polyvinyl Chloride, Flexible Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Initial Tear Strength; ASTM D1004-94 |
Saint-Gobain Tygon® 2001 Plasticizer Free Tubing Formulation Description: Tygon® 2001: Tygon® Plasticizer Free Tubing is a uniquely engineered product that offers the low compression set properties of a thermoset rubber. Tygon® Plasticizer Free Tub.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C; ASTM D624 |
Teknor Apex Telcar® TL-1522H Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Teknor Apex UNIPRENE® 7010-64 Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Tear Strength | 24.5 kN/m | 140 pli | at 25°C |
Daikin DAI-EL G-716 Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content Offers minimal compression set and excellent sealing. The copolymer type offers good compression set characteristics.Features: Minimal compression set and fast vulcanization.Information provided by.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | ASTM D624 |
Diamond Polymers Softflex® 4550 Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C, Vulcanizate, Press cured, TC95 +3min at 160°C |
Dow Nordel® IP 4570 General Purpose Compound FormulationNordel® IP 4570 |
|||
Tear Strength | 24.5 kN/m | 140 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ AF-10 Industrial Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 24.5 kN/m | 140 pli | B, cured 72 hrs @ RT |
ACC QM128 QSI Quantum Silicones 28 Durometer Condensation Cured Moldmaking Material QM 128 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and shelf-life stability. This material is an excellent choice f.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | Fill, Breaking Strength w/o Sizing |
3M Nextel™ AF-11 Aerospace Woven Fabric 312 Information provided by 3M |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 36-021 NATURAL Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:Specialty Thermoplastic ElastomerApplications: FDA (Food Contact)Processing Method: Injection MoldingInformation provided by PolyOne Corporation |
|||
Tear Strength | 24.5 kN/m | 140 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® IT 702 Thermoplastic Elastomer - SBC, Mineral Filled
(discontinued **) Description/Features:Multi-Purpose Thermoplastic ElastomerMineral FilledApplications:General PurposeMarket:Consumer GoodsIndustrialBuilding and ConstructionProcessing Method:Injection MoldingPolyOne.. |
|||
Tear Strength | 24.5 kN/m | 140 pli | die B; ASTM D624 |
G-2705 Styrene-based Biomedical Elastomer |
|||
Tear Strength | 24.5 kN/m | 140 pli | die B; ASTM D624 |
G-2712 Styrene-based Biomedical Elastomer |