Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Modulus of Rupture | 0.014715 - 0.016677 GPa @Temperature 1350 °C, Time 10800 sec |
2.1343 - 2.4188 ksi @Temperature 2460 °F, Time 3.00 hour |
|
Chosun Refractories HAPT-80S Plastic Refractory Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |