Modulus of Rupture 0.010791 GPa

@Temperature 1000 °C,
Time 10800 sec
1.5651 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories A80 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 1000 °C,
Time 10800 sec
1.5651 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSC-16 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 1000 °C,
Time 10800 sec
1.5651 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories HSC-16RA Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 1500 °C,
Time 10800 sec
1.5651 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories HSC-16RA Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 110 °C,
Time 86400 sec
1.5651 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories HSC-17 Dense and High-Strength Castable, Credens
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 1500 °C,
Time 10800 sec
1.5651 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories LPCT-16DS Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 110 °C,
Time 86400 sec
1.5651 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories LPCT-17PI Lance Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 110 °C,
Time 86400 sec
1.5651 ksi

@Temperature 230 °F,
Time 24.0 hour
Chosun Refractories SFC-165 High-Alumina Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 1000 °C,
Time 10800 sec
1.5651 ksi

@Temperature 1830 °F,
Time 3.00 hour
Chosun Refractories SW88 Special High-Density Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Modulus of Rupture 0.010791 GPa

@Temperature 1500 °C,
Time 10800 sec
1.5651 ksi

@Temperature 2730 °F,
Time 3.00 hour
Chosun Refractories TCH-165Y Torpedo Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).