Material Notes:
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Mechanical Properties Metric English Comments
Modulus of Rupture 0.010791 GPa

@Temperature 110 °C,
Time 86400 sec
1.5651 ksi

@Temperature 230 °F,
Time 24.0 hour
0.011772 GPa

@Temperature 1000 °C,
Time 10800 sec
1.7074 ksi

@Temperature 1830 °F,
Time 3.00 hour
0.012753 GPa

@Temperature 1350 °C,
Time 10800 sec
1.8497 ksi

@Temperature 2460 °F,
Time 3.00 hour
Compressive Strength 53.9 MPa

@Temperature 110 °C,
Time 86400 sec
7820 psi

@Temperature 230 °F,
Time 24.0 hour
Cold Crushing Strength
78.5 MPa

@Temperature 1000 °C,
Time 10800 sec
11400 psi

@Temperature 1830 °F,
Time 3.00 hour
Cold Crushing Strength
83.4 MPa

@Temperature 1350 °C,
Time 10800 sec
12100 psi

@Temperature 2460 °F,
Time 3.00 hour
Cold Crushing Strength
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1650 °C
3000 °F
limited
Shrinkage -0.0300 %

@Temperature 110 °C,
Time 86400 sec
-0.0300 %

@Temperature 230 °F,
Time 24.0 hour
0.12 %

@Temperature 1350 °C,
Time 10800 sec
0.12 %

@Temperature 2460 °F,
Time 3.00 hour
Component Elements Properties Metric English Comments
Al2O3 61 %
61 %
SiO2 34 %
34 %
Descriptive Properties Value Comments
Installation Method Self Flowing
Material Required for Estimating(kg/?) 2,450
Water Required for Casting(%) 7.3-7.7