Mechanical Properties Metric English Comments
Puncture Energy 1.50 - 1.50 J

@Temperature -30.0 - -30.0 °C
1.11 - 1.11 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.50 J Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Puncture Energy 1.50 - 1.80 J

@Temperature -30.0 - -30.0 °C
1.11 - 1.33 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.65 J Grade Count:2
Overview of materials for Nylon 6, Glass/Mineral Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values..
Puncture Energy 1.50 J

@Temperature -30.0 °C
1.11 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance
Puncture Energy 1.50 J

@Temperature -30.0 °C
1.11 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BKV 15 G H2.0 900051 Copolyamide, 15% Glass Fiber
CoPA, injection molding grade, 15% glass fibers, better surface resistance to alcoholic calcium chloride-solution than BKV 15 H2.0, good heat-ageing resistance
Puncture Energy 1.50 J

@Temperature -30.0 °C
1.11 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6, 40% Glass Fiber + Mineral
PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance
Puncture Energy 1.50 J

@Temperature -30.0 °C
1.11 ft-lb

@Temperature -22.0 °F
Conditioned; ISO 6603-2
Lanxess Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6, 40% Glass Fiber + Mineral
PA 6, injection molding grade, 40% glass fibers/mineral, good heat-ageing resistance
Puncture Energy 1.50 J
1.11 ft-lb
ASTM 5748
Borealis Borstar® FB1460 HDPE for Film
Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utiliz..
Puncture Energy 1.50 J
1.11 ft-lb
45N; ASTM D5748
Borealis FS1560 High Density Polyethylene
FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and bala..
Puncture Energy 1.50 J
1.11 ft-lb
45N; ASTM D5748
Borealis FS1470 High Density Polyethylene
FS1470 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1470 have high impact and tensile strength, and bala..
Puncture Energy 1.50 J
1.11 ft-lb
ISO 6603-2
Lanxess Pocan® B 3215 000000 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding
Puncture Energy 1.50 J

@Temperature -30.0 °C
1.11 ft-lb

@Temperature -22.0 °F
ISO 6603-2
Lanxess Pocan® B 3215 000000 PBT, 10% Glass Fiber
PBT, 10% glass fibers, injection molding
Copyright © lookpolymers.com All Rights Reserved