Material Notes:
Borstar FB1460 is a high-density polyethylene film grade, which combines superior physical properties with excellent processability. Due to the high density, the material properties are best utilized by processing at HDPE conditions. Film made of Borstar FB1460 gives a strong and stiff film with high consistency. Borstar FB1460 contains antioxidant.Borstar FB1460 is particularly suitable for applications where outstanding and well-balanced mechanical properties are required, such as industrial liners, carrier bags and heavy duty bags.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.946 g/cc
0.0342 lb/in³
ISO 1183
Melt Flow 0.20 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.20 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
High Load Melt Index 6.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
6.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 300 %
300 %
ISO 527-3
Film Elongation at Break, TD 450 %
450 %
ISO 527-3
Secant Modulus, MD 0.600 GPa
87.0 ksi
0.05-1.05%; ISO 527-3
Secant Modulus, TD 0.700 GPa
102 ksi
0.05-1.05%; ISO 527-3
Impact 38
38
Puncture Resistance, force (N); ASTM 5748
Puncture Energy 1.50 J
1.11 ft-lb
ASTM 5748
Tear Strength, Total 0.200 N
0.0450 lb (f)
MD; ISO 6383/2
1.00 N
0.225 lb (f)
TD; ISO 6383/2
Elmendorf Tear Strength, MD 1.36 g/micron
34.5 g/mil
ISO 6383/2
Elmendorf Tear Strength, TD 20.38 g/micron
517.7 g/mil
ISO 6383/2
Dart Drop 30.0 g/micron
762 g/mil
ISO 7765/1
Film Tensile Strength at Break, MD 75.0 MPa
10900 psi
ISO 527-3
Film Tensile Strength at Break, TD 60.0 MPa
8700 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point >= 131 °C
>= 268 °F
ISO 11357/03
Vicat Softening Point 125 °C
257 °F
A (10N); ISO 306