Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.14 - 1.75 g/cc
0.0412 - 0.0632 lb/in³
Average value: 1.45 g/cc Grade Count:186
Filler Content 10.0 - 44.0 %
10.0 - 44.0 %
Average value: 31.5 % Grade Count:30
Water Absorption 0.0900 - 8.00 %
0.0900 - 8.00 %
Average value: 3.43 % Grade Count:89
Moisture Absorption at Equilibrium 0.800 - 5.70 %
0.800 - 5.70 %
Average value: 1.99 % Grade Count:73
Water Absorption at Saturation 3.50 - 5.00 %
3.50 - 5.00 %
Average value: 4.26 % Grade Count:5
Viscosity Test 95.0 - 160 cm³/g
95.0 - 160 cm³/g
Average value: 138 cm³/g Grade Count:9
Linear Mold Shrinkage 0.000500 - 0.0150 cm/cm
0.000500 - 0.0150 in/in
Average value: 0.00466 cm/cm Grade Count:151
Linear Mold Shrinkage, Transverse 0.000800 - 0.0150 cm/cm
0.000800 - 0.0150 in/in
Average value: 0.00824 cm/cm Grade Count:67
Melt Flow 3.00 - 116 g/10 min
3.00 - 116 g/10 min
Average value: 35.7 g/10 min Grade Count:24
Mechanical Properties Metric English Comments
Hardness, Rockwell M 78.0 - 90.0
78.0 - 90.0
Average value: 86.0 Grade Count:3
Hardness, Rockwell R 116 - 122
116 - 122
Average value: 121 Grade Count:36
Ball Indentation Hardness 90.0 - 320 MPa
13100 - 46400 psi
Average value: 194 MPa Grade Count:5
Tensile Strength, Ultimate 45.0 - 174 MPa
6530 - 25200 psi
Average value: 102 MPa Grade Count:142
25.0 - 178 MPa

@Temperature -40.0 - 150 °C
3630 - 25800 psi

@Temperature -40.0 - 302 °F
Average value: 66.1 MPa Grade Count:9
25.0 - 145 MPa

@Temperature -30.0 - 120 °C
3630 - 21000 psi

@Temperature -22.0 - 248 °F
Average value: 66.1 MPa Grade Count:1
25.0 - 145 MPa

@Strain 1.00 - 10.0 %
3630 - 21000 psi

@Strain 1.00 - 10.0 %
Average value: 66.1 MPa Grade Count:1
Tensile Strength, Yield 40.0 - 186 MPa
5800 - 27000 psi
Average value: 103 MPa Grade Count:48
Elongation at Break 1.00 - 183 %
1.00 - 183 %
Average value: 4.88 % Grade Count:166
1.80 - 25.0 %

@Temperature -40.0 - 150 °C
1.80 - 25.0 %

@Temperature -40.0 - 302 °F
Average value: 6.51 % Grade Count:7
Elongation at Yield 1.80 - 22.6 %
1.80 - 22.6 %
Average value: 5.20 % Grade Count:13
Modulus of Elasticity 0.600 - 12.1 GPa
87.0 - 1750 ksi
Average value: 6.84 GPa Grade Count:104
1.70 - 10.79 GPa

@Temperature -100 - 200 °C
247 - 1565 ksi

@Temperature -148 - 392 °F
Average value: 4.65 GPa Grade Count:9
Flexural Yield Strength 50.0 - 261 MPa
7250 - 37800 psi
Average value: 166 MPa Grade Count:111
70.0 - 245 MPa

@Temperature -40.0 - 90.0 °C
10200 - 35500 psi

@Temperature -40.0 - 194 °F
Average value: 137 MPa Grade Count:2
Flexural Modulus 0.650 - 14.1 GPa
94.3 - 2050 ksi
Average value: 7.23 GPa Grade Count:127
2.40 - 8.40 GPa

@Temperature -40.0 - 120 °C
348 - 1220 ksi

@Temperature -40.0 - 248 °F
Average value: 4.30 GPa Grade Count:3
Compressive Yield Strength 89.6 - 159 MPa
13000 - 23100 psi
Average value: 119 MPa Grade Count:8
Shear Modulus >= 0.696 GPa

@Temperature -100 - 200 °C
>= 101 ksi

@Temperature -148 - 392 °F
Average value: 2.06 GPa Grade Count:1
Izod Impact, Notched 0.267 - 1.85 J/cm
0.500 - 3.47 ft-lb/in
Average value: 0.649 J/cm Grade Count:71
0.280 - 0.700 J/cm

@Temperature -40.0 - -20.0 °C
0.525 - 1.31 ft-lb/in

@Temperature -40.0 - -4.00 °F
Average value: 0.321 J/cm Grade Count:4
0.186865 - 0.186865 J/cm

@Temperature -40.0 - -40.0 °C
0.350075 - 0.350075 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.321 J/cm Grade Count:2
0.186865 - 0.186865 J/cm

@Thickness 3.17 - 3.17 mm
0.350075 - 0.350075 ft-lb/in

@Thickness 0.125 - 0.125 in
Average value: 0.321 J/cm Grade Count:2
Izod Impact, Unnotched 3.74 J/cm - NB
7.00 ft-lb/in - NB
Average value: 5.76 J/cm Grade Count:17
Izod Impact, Notched (ISO) 2.40 - 16.0 kJ/m²
1.14 - 7.61 ft-lb/in²
Average value: 5.97 kJ/m² Grade Count:55
3.00 - 10.0 kJ/m²

@Temperature -40.0 - -30.0 °C
1.43 - 4.76 ft-lb/in²

@Temperature -40.0 - -22.0 °F
Average value: 5.65 kJ/m² Grade Count:15
Izod Impact, Unnotched (ISO) 20.0 - 82.0 kJ/m²
9.52 - 39.0 ft-lb/in²
Average value: 40.3 kJ/m² Grade Count:7
45.0 - 50.0 kJ/m²

@Temperature -30.0 - -30.0 °C
21.4 - 23.8 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 47.5 kJ/m² Grade Count:2
Charpy Impact Unnotched 1.50 - 1000 J/cm²
7.14 - 4760 ft-lb/in²
Average value: 4.78 J/cm² Grade Count:77
1.30 - 999.9 J/cm²

@Temperature -40.0 - 30.0 °C
6.19 - 4759 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 3.55 J/cm² Grade Count:49
Charpy Impact, Notched 0.200 - 1.60 J/cm²
0.952 - 7.61 ft-lb/in²
Average value: 0.682 J/cm² Grade Count:83
0.200 - 1.00 J/cm²

@Temperature -40.0 - 30.0 °C
0.952 - 4.76 ft-lb/in²

@Temperature -40.0 - 86.0 °F
Average value: 0.478 J/cm² Grade Count:50
Puncture Energy 1.50 - 1.80 J

@Temperature -30.0 - -30.0 °C
1.11 - 1.33 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 1.65 J Grade Count:2
Thermal Properties Metric English Comments
CTE, linear 14.4 - 110 µm/m-°C
8.00 - 61.1 µin/in-°F
Average value: 35.9 µm/m-°C Grade Count:53
CTE, linear, Transverse to Flow 34.0 - 100 µm/m-°C
18.9 - 55.6 µin/in-°F
Average value: 66.3 µm/m-°C Grade Count:24
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 - 1.00e+15 ohm-cm
1.00e+9 - 1.00e+15 ohm-cm
Average value: 2.37e+14 ohm-cm Grade Count:72
Surface Resistance 1.00e+10 - 1.00e+16 ohm
1.00e+10 - 1.00e+16 ohm
Average value: 3.60e+14 ohm Grade Count:36
Dielectric Constant 3.00 - 14.0
3.00 - 14.0
Average value: 5.37 Grade Count:48
Dielectric Strength 11.8 - 90.0 kV/mm
300 - 2290 kV/in
Average value: 27.8 kV/mm Grade Count:50
Dissipation Factor 0.00380 - 0.400
0.00380 - 0.400
Average value: 0.0895 Grade Count:36
Dielectric Loss Index 0.0200 - 0.200
0.0200 - 0.200
Average value: 0.110 Grade Count:6
Arc Resistance 100 - 130 sec
100 - 130 sec
Average value: 119 sec Grade Count:6
Comparative Tracking Index 300 - 600 V
300 - 600 V
Average value: 501 V Grade Count:45