Material Notes:
FS1560 is a high density polyethylene film grade which combine excellent extrusion behavior with superior mechanical properties. Films made of FS1560 have high impact and tensile strength, and balanced tear properties. Applications FS1560 has been developed especially for applications like: heavy-duty sacks, refuse sacks and liners, and carrier-bag film. FS1560 contains antioxidant.Information provided by Borealis AG
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
ISO 1183
Melt Flow 0.30 g/10 min

@Load 5.00 kg,
Temperature 190 °C
0.30 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ISO 1133
9.0 g/10 min

@Load 21.6 kg,
Temperature 190 °C
9.0 g/10 min

@Load 47.6 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD 250 %
250 %
ISO 527-3
Film Elongation at Break, TD 300 %
300 %
ISO 527-3
Tensile Modulus 1.00 GPa
145 ksi
MD; ASTM D882-A
1.10 GPa
160 ksi
TD; ASTM D882-A
Puncture Energy 1.50 J
1.11 ft-lb
45N; ASTM D5748
Elmendorf Tear Strength MD 20.387 g
20.387 g
ISO 6383/2
Elmendorf Tear Strength TD 30.58 g
30.58 g
ISO 6383/2
Dart Drop Test 350 g
0.772 lb
ISO 7765-1
Film Tensile Strength at Break, MD 50.0 MPa
7250 psi
ISO 527-3
Film Tensile Strength at Break, TD 55.0 MPa
7980 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 133 °C
271 °F
ISO 11357-3
Vicat Softening Point 127 °C
261 °F
ISO 306
Processing Properties Metric English Comments
Melt Temperature 210 - 230 °C
410 - 446 °F