Polymer Property : Flexural Modulus = 95.0 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.655 GPa
95.0 ksi
ASTM D790
Huntsman Rexell® H2109 Injection Molding LLDPE  (discontinued **)
Linear-low high density injection molding.Features: High flow, good ESCR.Applications: General purpose molding, housewares.Information provided by Huntsman Corporation
Flexural Modulus 0.655 GPa
95.0 ksi
ASTM D790
NOVA Chemicals Sclair® 8405 BK, 8405GBK MDPE Rotational Molding Resin  (discontinued **)
Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer.
Flexural Modulus 0.655 GPa
95.0 ksi
ASTM D790
NOVA Chemicals Sclair® 8405 UV8D, 8405G UV8D MDPE Rotational Molding Resin  (discontinued **)
Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer.
Flexural Modulus 0.655 GPa
95.0 ksi
ASTM D790
Global TPO-65D TPO Grade
Data provided by Global Polymers Corporation.
Flexural Modulus 0.655 GPa
95.0 ksi
Tangent-Method 1; ASTM D790
Ineos G36-10-150 HDPE
G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes...
Flexural Modulus 0.655 GPa
95.0 ksi
ASTM D790
ScanTube FEP Tubing
Information provided by ScanTube, Inc.
Flexural Modulus 0.655 GPa
95.0 ksi
ASTM D790
ScanTube MFA Tubing
Information provided by ScanTube, Inc.
Flexural Modulus 0.655 GPa
95.0 ksi
At 2 mm/min; ASTM D790
Borealis Borecene Compact™ RM7406 Black Metallocene Linear Polyethylene for Rotational Molding
Borecene Compact RM7406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides ..
Flexural Modulus 0.655 GPa
95.0 ksi
At 2 mm/min; ASTM D790
Borealis Borecene Compact™ RM8406 Black Linear Polyethylene for Rotational Molding
Borecene Compact RM8406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides ..
Flexural Modulus 0.655 GPa
95.0 ksi
CMW® ELKONITE® 2050C Copper Tungsten Contact Material ASTM B702, Class A, infiltrated
Uses: Arcing and current carrying electrical contacts. Information provided by CMW Inc.
Flexural Modulus 0.655 GPa
95.0 ksi
CMW® ELKONITE® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated
For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc.
Flexural Modulus >= 0.655 GPa
>= 95.0 ksi
ASTM D790
Buckeye Polymers BP FLEX D6017 T BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Processing Method: Injection Mold..