Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.655 GPa | 95.0 ksi | ASTM D790 |
Huntsman Rexell® H2109 Injection Molding LLDPE
(discontinued **) Linear-low high density injection molding.Features: High flow, good ESCR.Applications: General purpose molding, housewares.Information provided by Huntsman Corporation |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | ASTM D790 |
NOVA Chemicals Sclair® 8405 BK, 8405GBK MDPE Rotational Molding Resin
(discontinued **) Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | ASTM D790 |
NOVA Chemicals Sclair® 8405 UV8D, 8405G UV8D MDPE Rotational Molding Resin
(discontinued **) Features: Good ESCR, high impact strength.Applications: Spray tanks.Data provided by the manufacturer. |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | ASTM D790 |
Global TPO-65D TPO Grade Data provided by Global Polymers Corporation. |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | Tangent-Method 1; ASTM D790 |
Ineos G36-10-150 HDPE G36-10-150 is a medium density hexene copolymer polyethylene resin designed for the blown geomembrane sheet process. This resin is especially well suited for the production of textured geomembranes... |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | ASTM D790 |
ScanTube FEP Tubing Information provided by ScanTube, Inc. |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | ASTM D790 |
ScanTube MFA Tubing Information provided by ScanTube, Inc. |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene Compact™ RM7406 Black Metallocene Linear Polyethylene for Rotational Molding Borecene Compact RM7406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | At 2 mm/min; ASTM D790 |
Borealis Borecene Compact™ RM8406 Black Linear Polyethylene for Rotational Molding Borecene Compact RM8406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides .. |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | |
CMW® ELKONITE® 2050C Copper Tungsten Contact Material ASTM B702, Class A, infiltrated Uses: Arcing and current carrying electrical contacts. Information provided by CMW Inc. |
|||
Flexural Modulus | 0.655 GPa | 95.0 ksi | |
CMW® ELKONITE® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Flexural Modulus | >= 0.655 GPa | >= 95.0 ksi | ASTM D790 |
Buckeye Polymers BP FLEX D6017 T BLK Thermoplastic Polyolefin Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Processing Method: Injection Mold.. |