Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Huntsman Rexell® H2109 Injection Molding LLDPE  (discontinued **)

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman Rexell® H2109 Injection Molding LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Linear-low high density injection molding.Features: High flow, good ESCR.Applications: General purpose molding, housewares.Information provided by Huntsman Corporation
Physical Properties Metric English Comments
Density 0.950 g/cc
0.0343 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 63
63
ASTM D2240
Tensile Strength, Ultimate 13.0 MPa
1890 psi
ASTM D638
Tensile Strength, Yield 21.0 MPa
3050 psi
ASTM D638
Elongation at Break 670 %
670 %
ASTM D638
Modulus of Elasticity 0.786 GPa
114 ksi
ASTM D638
Flexural Modulus 0.655 GPa
95.0 ksi
ASTM D790
Thermal Properties Metric English Comments
Vicat Softening Point 125 °C
257 °F
ASTM D1525