Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Borealis Borecene Compact™ RM7406 Black Metallocene Linear Polyethylene for Rotational Molding

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer Borealis
Trade Name Borecene Compact™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Borealis Borecene Compact™ RM7406 Black Metallocene Linear Polyethylene for Rotational Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Borecene Compact RM7406 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides an ideal balance of flow and physical properties. Borecene Compact RM7406 is a black version of Borecene RM7403, suitable for high strength applications. Borecene Compact RM7406 is delivered as new technology powder.Borecene Compact RM7406 contains 0.5% Carbon Black, which is compounded into the polymer. In addition the grade contains an UV stabilizer which gives excellent UV-stability. The polymer contains long-term antioxidant.Information provided by the Manufacturer.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
Base Resin; ASTM D1505
ESCR 10% Igepal® >= 200 hour
>= 200 hour
ARM Method
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa
3200 psi
At 50 mm/min; ASTM D683 IV
Flexural Modulus 0.655 GPa
95.0 ksi
At 2 mm/min; ASTM D790
Dart Drop Total Energy 200.0 J/cm
0.3746 ft-lb/mil
Instrumented Falling Weight (-4°F/-20°C); ASTM D3763
Dart Drop 152 g/micron
3860 g/mil
Instrumented Falling Weight (-4°F/-20°C); ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 72.0 °C
162 °F
ASTM D648
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746