BCC Products BC 7009-2 Epoxy Casting

Category Polymer , Thermoset , Epoxy
Manufacturer BCC Products
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BCC Products BC 7009-2 Epoxy Casting.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in metal or conductive-type molds can successfully be achieved as well. Ideal for stretch forms, patterns, dies, molds, duplications, prototypes, etc.Information provided by BCC Products, Inc.
Physical Properties Metric English Comments
Specific Gravity 2.27 g/cc
2.27 g/cc
Brookfield Viscosity 35000 cP

@Temperature 23.9 °C
35000 cP

@Temperature 75.0 °F
Mixed
Linear Mold Shrinkage 0.00090 cm/cm
0.00090 in/in
Mechanical Properties Metric English Comments
Hardness, Shore D 85

@Temperature 23.9 °C
85

@Temperature 75.0 °F
Tensile Strength, Ultimate 37.2 MPa
5400 psi
Flexural Strength 51.0 MPa
7400 psi
Flexural Modulus 5.58 GPa
810 ksi
Compressive Strength 86.9 MPa
12600 psi
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 50.6 °C
123 °F
Processing Properties Metric English Comments
Cure Time 1440 min

@Temperature 24.0 °C
24.0 hour

@Temperature 75.2 °F
Pot Life 240 min

@Temperature 24.0 °C
240 min

@Temperature 75.2 °F
15 lb. mass
Descriptive Properties Value Comments
Machinability Good
Mix Ratio 12:1 by weight, 4.5:1 by volume, resin/harder