Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled , Nylon 66, Heat Stabilized , Nylon 66, Mineral Filled, Impact Grade
Manufacturer Techmer ES
Trade Name HiFill®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.70 %

@Time 86400 sec
0.70 %

@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0090 cm/cm

@Thickness 3.17 mm
0.0090 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Yield 91.0 MPa
13200 psi
ASTM D638
Elongation at Break 15 %
15 %
ASTM D638
Flexural Strength 138 MPa
20000 psi
ASTM D790
Flexural Modulus 5.58 GPa
810 ksi
ASTM D790
Izod Impact, Notched 0.694 J/cm

@Thickness 3.17 mm
1.30 ft-lb/in

@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 7.47 J/cm

@Thickness 3.17 mm
14.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 7.20 µm/m-°C
4.00 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 232 °C
450 °F
Unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 90.6 °C
195 °F
Unannealed; ASTM D648
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
ASTM D257
Dielectric Strength 18.1 kV/mm
460 kV/in
Method A (Short-Time); ASTM D149