Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
Nylene® PA6 Mineral Filled 6240 HS Nylon 6 40% MR; Dry as molded.ALM, Nylene Canada, and Custom Resins are all operting companies of Polymeric Resources Corporation. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
PolyOne Edgetek® PC-20GF/000 Polycarbonate (PC) Information provided by PolyOne |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
PolyOne Edgetek® PF-20GF/000 Polysulfone (PSU) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
PolyOne Geon™ 80520 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
LNP Thermocomp® EF-1002 EP BK8-114 Polyetherimide, Glass Fiber Reinforcement
(discontinued **) Features: Good ProcessabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are.. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU)
(Unverified Data**) Udel GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resi.. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11 (Asia Pacific) LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing Glass Fiber, Graphite Powder. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
Solvay Specialty Polymers Ryton® XE5515BL Polyphenylene Sulfide Alloy (PPS Alloy), 15% Glass Fiber Ryton® XE5515BL 15% glass fiber reinforced polyphenylene sulfide alloy compound provides excellent mechanical strength and chemical resistance at elevated temperatures and is suitable for extrusi.. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | ASTM D790 |
Solvay Specialty Polymers Udel® GF-120 Polysulfone (PSU), Glass Fiber Udel® GF-120, resin is a 20% glass fiber reinforced polysulfone compound. Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical .. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Stat-kon PE002 PA 6 (Asia Pacific) LNP* Stat-kon* PE002 is a compound based on Nylon 6 resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the Asia P.. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX4605 PPE+PS PPE+PS blend. 20% Glass reinforced. High heat. Dimensional stability. Suitable for automotive and E/E applications. |
|||
Flexural Modulus | 5.52 GPa | 801 ksi | |
Reliance Industries Polypropylene - 40% Glass filled Information provided by Reliance Industries |