Material Notes:
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for elevated service temperature environments, high-modulus / structural materials for load-bearing and high-strength applications and flame-retardant products. These compounds are based on select engineering thermoplastic resins that are compounded with reinforcing additives such as carbon fiber, glass fiber and glass beads.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.38 g/cc
1.38 g/cc
ASTM D792
Water Absorption 0.20 %
0.20 %
@ 24 hrs; ASTM D570
Water Absorption at Saturation 0.60 %
0.60 %
ASTM D570
Linear Mold Shrinkage, Flow 0.0030 cm/cm
0.0030 in/in
ASTM D955
0.0030 - 0.0040 cm/cm
0.0030 - 0.0040 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 92
92
ASTM D785
Tensile Strength at Break 103 MPa
14900 psi
Type I, 5.1 mm/min; ASTM D638
Elongation at Break 3.0 %
3.0 %
Type I, 5.1 mm/min; ASTM D638
Tensile Modulus 5.52 GPa
801 ksi
Type I, 5.1 mm/min; ASTM D638
Flexural Strength 152 MPa
22000 psi
ASTM D790
Flexural Modulus 5.52 GPa
801 ksi
ASTM D790
Compressive Strength 138 MPa
20000 psi
ASTM D695
Shear Strength 62.7 MPa
9090 psi
ASTM D732
Izod Impact, Notched 0.690 J/cm

@Thickness 6.35 mm,
Temperature 23.0 °C
1.29 ft-lb/in

@Thickness 0.250 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 29.0 µm/m-°C
16.1 µin/in-°F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 185 °C

@Thickness 3.18 mm
365 °F

@Thickness 0.125 in
Annealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 179 °C

@Thickness 3.18 mm
354 °F

@Thickness 0.125 in
Annealed; ASTM D648
Flammability, UL94 V-0
V-0
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 338 - 371 °C
640 - 700 °F
Mold Temperature 93.3 - 149 °C
200 - 300 °F
Drying Temperature 135 °C
275 °F
Dry Time 2.00 hour
2.00 hour
Descriptive Properties Value Comments
Filler / Reinforcement Glass Fiber Reinforcement, 20% Filler by Weight
Forms Pellets
Generic Material PSU
Generic Name Polysulfone (PSU)
Regional Availability Africa & Middle East
Asia Pacific
Europe
South America
RoHS Compliance RoHS Compliant