Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.76 GPa | 1270 ksi | ASTM D790 |
LNP Thermocomp® LF-1004 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Flexural Modulus | 8.76 GPa | 1270 ksi | ASTM D790 |
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 8.76 GPa | 1270 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOTUF CF007IXP PS LNP* Thermotuf* CF007IXP is a compound based on Polystyrene containing glass fiber. Characteristics of this grade are: High Impact. |
|||
Flexural Modulus | 8.76 GPa | 1270 ksi | ASTM Test |
BASF Petra® 130 BK-112 30% Glass Filled PET Petra 130 BK-112 is a 30% glass fiber reinforced, black pigmented polyethylene terephthalate injection molding compound. It exhibits a combination of performance properties including good strength .. |
|||
Flexural Modulus | 8.76 GPa | 1270 ksi | ASTM D790 |
Applied Nanostructured Solutions Carbon NanoStructure Chopped Fiber Carbon NanoStructure (CNS) Chopped Fiber begins as a single-end glass roving product, such as E-CR glass, that is enhanced using a proprietary ANS process. Unique multiwall carbon nanotube-based CNS.. |
|||
Flexural Modulus | 8.76 GPa | 1270 ksi | ASTM D790 |
Asahi Kasei Thermylene® P7-45FG-0790 45% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Flexural Modulus | 8.76 GPa | 1270 ksi | ISO Data |
BASF Petra® 230 BK-112 22/13% Glass/Mineral Filled PET Petra 230 BK-112 is a 35% mineral and glass fiber reinforced, black pigmented, polyethylene terephthalate injection molding compound. It exhibits a very good combination of performance properties in.. |
|||
Flexural Modulus | 8.76 GPa | 1270 ksi | ASTM D790 |
LNP Thermocomp® JF-1006 EM Polyethersulfone, Glass Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Flexural Modulus | 8.76 GPa | 1270 ksi | ASTM D790 |
PlastxWorld CEVIAN® B2706 30% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |