Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Kasei Thermylene® P7-45FG-0790 45% Glass Fiber Reinforced, Heat Stabilized

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Glass Fiber Filler
Manufacturer Asahi Kasei
Trade Name Thermylene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermylene® P7-45FG-0790 45% Glass Fiber Reinforced, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.29 g/cc
1.29 g/cc
ASTM D792
Linear Mold Shrinkage 0.0030 cm/cm
0.0030 in/in
ASTM D955
Melt Flow 2.5 g/10 min
2.5 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 121 MPa
17500 psi
ASTM D638
Elongation at Yield 2.0 %
2.0 %
ASTM D638
Flexural Strength 165 MPa
24000 psi
ASTM D790
Flexural Modulus 8.76 GPa
1270 ksi
ASTM D790
Izod Impact, Notched 1.01 J/cm
1.90 ft-lb/in
ASTM D256
Izod Impact, Unnotched 7.47 J/cm
14.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 156 °C
313 °F
ASTM D648